Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 100 GPa | 14500 ksi | |
Goodfellow Aluminum-Copper/SiC Metal Matrix Composite Information provided by Goodfellow. |
|||
Tensile Modulus | 100 GPa | 14500 ksi | |
Goodfellow Aluminum-Lithium/SiC Metal Matrix Composite Information provided by Goodfellow. |