Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.93 GPa | 1440 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DFL369XF PC LNP* LUBRICOMP* DFL369XF is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Flame Retardant. |
|||
Tensile Modulus | 9.95 GPa @Temperature 23.0 °C |
1440 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® CE15330 NC010 PBT
(Unverified Data**) Crastin® CE15330 NC010 is a 30% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance.. |
|||
Tensile Modulus | 9.90 GPa | 1440 ksi | 1 mm/min; ISO 527-1,-2 |
Gromax BFG30-FH00B1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Modulus | 9.90 GPa | 1440 ksi | |
LATI Latilub 66-10T G/30-V0KB1 PA66, 10% Glass Fiber Reinforced, PTFE Filled, Flame Retardant Self-lubricating product based on Polyamide 66 (PA66). PTFE. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A.. |
|||
Tensile Modulus | 9.90 GPa | 1440 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218 V40 PA66, 40% glass fiber, Conditioned Description: Polyamide PA66, reinforced with 40% of glass fiber, heat stabilized for injection molding.Available in: Asia Pacific, Europe and North AmericaProduct Applications: TECHNYL A 218 V40 is .. |
|||
Tensile Modulus | 9.96 GPa | 1440 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP IFL36 PA6.12 LNP LUBRICOMP* IFL36 is a compound based on Nylon 6/12 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Tensile Modulus | 9.90 GPa | 1440 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP PFN16 PA 6 LNP* LUBRICOMP* PFN16 is a compound based on Nylon 6 resin containing 30% Glass Fiber, 2% MOS2. Added features of this material include: Wear Resistant. |
|||
Tensile Modulus | 9.94 GPa | 1440 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP QFN16 PA 6/10 LNP* LUBRICOMP* QFN16 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber, 5% MOS2. Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 9.90 GPa | 1440 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RFN16SXZ PA 66 LNP LUBRICOMP* RFN16SXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber, 5% MOS2. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
Tensile Modulus | 9.90 GPa | 1440 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 4000 PEI (Europe-Africa-Middle East) Glass fiber, PTFE, and Graphite filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 listing. |
|||
Tensile Modulus | 9.90 GPa | 1440 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON AE003 ABS (Europe-Africa-Middle East) LNP* STATKON* AE003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Carbon Fiber. Added features inclurde : Electrically Conductive. |
|||
Tensile Modulus | 9.90 GPa | 1440 ksi | 5 mm/min; ASTM D638 |
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire® AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This r.. |
|||
Tensile Modulus | 9.90 GPa | 1440 ksi | 5 mm/min; ASTM D638 |
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 res.. |
|||
Tensile Modulus | 9.95 GPa | 1440 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 8032UX PBT+PET VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Tensile Modulus | 9.95 GPa | 1440 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Asia Pacific) VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Tensile Modulus | 9.92 GPa | 1440 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DEL329E PC LNP* Stat-kon* DEL329E is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Flame Retardant, Wear Resi.. |
|||
Tensile Modulus | 9.90 GPa | 1440 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOTUF VF008 Super Tough Nylon LNP THERMOTUF* VF008 is a compound based on Super Tough Nylon resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Tensile Modulus | 9.90 GPa | 1440 ksi | ISO 527 |
Polyram RamSter PF306G6 PBT, 30% Glass Fiber 30% Glass fiber reinforced, low viscosity PBT for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 9.90 GPa | 1440 ksi | ASTM D638 |
Plenco 4300 Phenolic, Granular, Injection Molded PLENCO 04300 is a heat resistant, mineral filled phenolic molding compound offering optimum cure characteristics and excellent dimensional stability. It is formulated for wiring devices and electric.. |
|||
Tensile Modulus | 9.90 GPa | 1440 ksi | ASTM D638 |
Plenco 4504 Phenolic, Granular, Injection Molded Plenco 04504 is a renumber of Plaslok 504. Plenco 04504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding c.. |
|||
Tensile Modulus | 9.90 GPa | 1440 ksi | ISO 527-1/-2 |
DSM Arnite® TV4 461 (PBT+PET)-GF30 30% Glass Reinforced |
|||
Tensile Modulus | 9.90 GPa | 1440 ksi | ISO 527-1/-2 |
DSM Arnite® TV4 461 KL (PBT+PET)-GF30 30% Glass Reinforced, Heat Stabilized, UV Stabilized, Excellent Surface Properties |
|||
Tensile Modulus | 9.95 GPa | 1440 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® CE15330 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® CE15330 NC010 is a 30% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V.. |
|||
Tensile Modulus | 9.94 GPa @Temperature -110 °C |
1440 ksi @Temperature -166 °F |
DAM; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® EFE6053 BK413 Nylon 66
(Unverified Data**) 40% Mineral/Glass Reinforced Polyamide 66 Minlon EFE6053 BK413 is a 40% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance P.. |
|||
Tensile Modulus | 9.90 GPa | 1440 ksi | 1mm/min; ISO 527 |
BASF Ultradur S 4090 G6 LS High Speed BK15077 30% Glass Filled PBT Ultradur S 4090 G6 LS High Speed BK15077 is a high flow, fast cycling with low warpage, 30% glass filled injection molding PBT. |
|||
Tensile Modulus | 9.90 GPa | 1440 ksi | ISO 527-1/-2 |
DSM Arnite® TV4 261 KL PBT-GF30 30% Glass Reinforced, Light Stabilized |
|||
Tensile Modulus | 9.90 GPa | 1440 ksi | |
Radici Radilon® A RV350 (cond) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Tensile Modulus | 9.93 GPa | 1440 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DFL369XF PC (Asia Pacific) LNP* Lubricomp* DFL369XF is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retardant. |
|||
Tensile Modulus | 9.90 GPa | 1440 ksi | ASTM D638 |
Plenco 1506 Polyester, Briquette, Injection Molded PLENCO 01506 is a mineral and cellulose filled granular polyester molding compound, with glass fiber reinforcement for improved mechanical strength properties. 01506 offers excellent electrical prop.. |
|||
Tensile Modulus | 9.90 GPa | 1440 ksi | 1mm/min; ISO 527 |
BASF Ultramid® N-265 NF3001 40% Mineral Filled PA66 (Dry) Ultramid N-265 NF3001 is a general purpose, 40% mineral reinforced PA6/6 that provides excellent flatness and dimensional stability in injection molding. |