Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.990 GPa | 144 ksi | Secant; ASTM D638 |
NOVA Chemicals Novapol® HE-D250A HDPE Extrusion Resin
(discontinued **) Features: Excellent ESCR and toughness, good processability.Applications: conduit, corrugated pipe.Data provided by the manufacturer. |
|||
Tensile Modulus | 0.993 GPa | 144 ksi | ASTM D638 |
CPC - Vycom CELTEC MARINE™ Expanded Foam PVC Polyvinyl Chloride Celtec Marine is made from rigid expanded foam polyvinyl chloride (PVC) material whose combination of features makes it ideal for wood trim and plywood replacement in boat manufacturing. Its closed .. |