Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.80 GPa | 1420 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID® 6 GF 30 AS PA6 reinforced with glass fiber, anti-static agent PA 6 for injection molding, reinforced with 30% glass fiber, contains antistatic agent for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric.. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | |
Plastcom SLOVASTER® B/A GF 30 PBT, 30% glass fibre FeaturesPBT/ASA for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and ben.. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® BKV 50 H2.0 901510 Nylon 6, 50% Glass Fiber PA 6, injection molding grade, 50% glass fibers, good heat-ageing resistance |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP JFL36 PES (Europe-Africa-Middle East) LNP* Lubricomp* JFL36 is a compound based on Polyethersulfone resin containing Glass Fiber, PTFE. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | ISO 527 Type 1A |
Solvay TECHNYL® B 216 V30 Black 3 N PA66, 30% glass fiber, DRY Description: Copolyamide 66/6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHNYL® B 216 V30 is used in all sectors of in.. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | ISO 527 Type 1A |
Solvay TECHNYL® B 218 V30 Black 21 N PA66, 30% glass fiber, DRY Description: Copolyamide PA66/6, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHNYL® B 218 V30 is used i.. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | ISO 527 Type 1A |
Solvay TECHNYL® B 218L V30 Black 44 N PA66, 30% glass fiber, DRY Description: Copolyamide 66/6, reinforced with 30% of glass fiber, for injection molding, heat stabilized with improved UV ageing resistance.Available in: Asia Pacific, Europe and Latin AmericaProdu.. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RFG16 PA 66 (Europe-Africa-Middle East) LNP* LUBRICOMP* RFG16 is a compound based on PA 66 resin containing Glass Fiber, Graphite. Added features include: Internally Lubricated. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36XXZ PA 66 (Asia Pacific) LNP Lubricomp is a compound based on PA66 resin containing glass fiber, PTFE. It is an internally lubricated compound that provide excellent chemical resistance, strength and wear/friction propertie.. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RFP36 PA 66 (Asia Pacific) LNP* Lubricomp* RFP36 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE, Silicone. Added features of this material include: Internally Lubricated. This product is also known as Lub.. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RFP36S PA 66 LNP* LUBRICOMP* RFP36S is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 2412EPR PEI (Asia Pacific) 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the As.. |
|||
Tensile Modulus | 9.81 GPa | 1420 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DX09315C PC (Asia Pacific) LNP* Stat-Kon* DX09315C is carbon fiber filled polycarbonate composite with good flow ability, and high level of cleanliness for the most demanding application. A unique feature of this material is .. |
|||
Tensile Modulus | 9.79 GPa | 1420 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP JF006LXZ PES (Asia Pacific) LNP* Thermocomp* JF006LXZ is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Low Extractible. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON MV007SU PP (Europe-Africa-Middle East) LNP* VERTON * MV007SU is a compound based on PP resin containing Long Glass Fiber. Added features include; Chemically Coupled, Heat Stabilized, UV Stabilizedl. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON MV007SUP PP (Europe-Africa-Middle East) LNP* VERTON* MV007SUP is a compound based on PP resin containing Long Glass Fiber. Added features include; Chemically Coupled, Heat Stabilized, UV Stabilized. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON MV007U PP (Europe-Africa-Middle East) LNP* VERTON* MV007U is a compound based on PP resin containing Long Glass Fiber. Added features include; Chemically Coupled, Heat Stabilized, UV Stabilized. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP QFL36 PA 6/10 LNP LUBRICOMP* QFL36 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Tensile Modulus | 9.79 GPa | 1420 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RF006EUC PA 66 LNP* THERMOCOMP* RF006EUC is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include Easy Molding, UV Stabilized. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | ASTM-D790 |
Polyram PlusTek PA309G6 Nylon 6.6, 30% Glass Fiber 30% glass fiber reinforced, UV stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | ISO 527 |
Polyram RamLloy PFS301G6 ASA/PBT Alloy, 30% Glass Fiber 30% Glass fiber reinforced ASA/PBT alloy for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® FE5382 BK276 Nylon 612
(Unverified Data**) 33% Glass Reinforced Polyamide 612 Developed for Electrical and Electronics Applications Zytel FE5382 BK276 is a 33% glass fiber reinforced heat stabilized black polyamide 612 resin developed for el.. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam RF0055E PA66/6, 25% Glass Filled, Injection Molded Starflam RF0055E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z250EM)Information provided by Polym.. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® A3 GF 40 (1258) PA 6.6 Conditioned, 40% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | ISO 527-1/-2 |
BASF Ultradur® B 4300 G6 FC 30% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |
|||
Tensile Modulus | 9.79 GPa @Temperature -40.0 °C |
1420 ksi @Temperature -40.0 °F |
ISO Data |
BASF Ultramid® 8267G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid 8267G HS BK-102 is a heat stabilized, black pigmented, 40% mineral and glass fiber reinforced nylon 6 injection molding compound. It possesses a balance of engineering properties in combin.. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | ISO 527-1/-2 |
Lanxess Durethan® BKV 30 W1 000000 Nylon 6, 30% Glass Fiber PA 6, Injection molding grade, 30% glass fibers, weather stabilized |