Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 96.5 GPa | 14000 ksi | |
PSM Industries Pacific Sintered Metals Iron F-200-P Powdered Metal Low stressed mechanical components, Soft magnetic applications Equivalent MPIF Specification: F-0000-10Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Modulus | 96.5 GPa @Temperature 23.9 °C |
14000 ksi @Temperature 75.0 °F |
0° Direction, Dry; 325°F, 1000psi Cured; ASTM D638 |
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, 12K GA090 Uni Tape Reinforced Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock.. |