Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.65 GPa | 1400 ksi | ASTM D638 |
PolyOne LubriOne™ NN-30GF/10T WHT Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Modulus | 9.65 GPa | 1400 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne OnForce™ LFT UR-30 LGF/000 Natural Polyurethane, Unspecified (PUR, Unspecified) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Tensile Modulus | 9.65 GPa | 1400 ksi | same value from ASTM and ISO test. |
BASF Capron® GR30 30% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR30 is a 30% glass reinforced polyamide 6 injection molding compound. IT is also available in heat stabilized (Capron GR30 HS) and/or pigmented versions. The glass fiber reinforcement enhanc.. |
|||
Tensile Modulus | 9.65 GPa | 1400 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36ELH PC (Asia Pacific) LNP* Lubricomp* DFL36ELH is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Tensile Modulus | 9.68 GPa | 1400 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Tensile Modulus | 9.65 GPa | 1400 ksi | ASTM D638 |
Ecomass® 1700TU96 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Polyamide (PA) AlloyRigidInformation provided by Technical Po.. |
|||
Tensile Modulus | 9.65 GPa | 1400 ksi | 45° stress angle |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Unidirectional CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |
|||
Tensile Modulus | 9.65 GPa | 1400 ksi | ASTM D638 |
Ensinger Tecapeek® XP-97 Compression Molded PEEK Compound, 30% Graphite Filled Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Tensile Modulus | 9.65 GPa | 1400 ksi | ASTM D638 |
Ensinger Tecapeek® XP-98 Compression Molded PEEK Compound, 30% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |