Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.00 GPa | 1310 ksi | ASTM D638 |
Premix Premi-Glas® 2203-15 CR-SX-HT Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-15 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL.. |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | ISO 527-1,2 |
Qualchem Danamid FGFH-30 Polyamide 6, 30% Glass Fiber Reinforced with glass fiber. Heat stabilized, for long-lasting use at 120-140°C.Information provided by Qualchem Zrt. |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | ISO 527-2/1A |
Radici Raditer® B RVA 300 Polybutylene Terephthalate with 30% Glass fiber Raditer® B RVA is a range of glass fiber reinforced Polybutylene terephthalate blends for injection molding, with excellent dimensional stability, low warpage and good surface aspect.Information pr.. |
|||
Tensile Modulus | 9.00 GPa @Temperature 23.0 °C |
1310 ksi @Temperature 73.4 °F |
ISO 527-2 |
PolyOne Bergadur™ PB400 G30 H UF UV Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | Type I, 5.0 mm/min; ISO 527 |
PolyOne Edgetek® QT-30GF/000 Natural Syndiotactic Polystyrene (SPS) Information provided by PolyOne |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® A-1240 HS Polyphthalamide (PPA) Resin, 40% Mineral Reinforced, Dry As Molded
&nbs AMODEL A-1240 polyphthalamide (PPA) resins are 40% mineral filled resins that have high deflection temperature, flexural modulus, and tensile strength. They mold with low warpage, have excellent di.. |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | ISO 527 |
Nilit FRIANYL B63 HH-GV30 Nylon 6 for injection molding, 30% glass fiber reinforced Nylon 6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | ISO 527 |
Nilit RECONYL A GV30 Recycled nylon 6.6 for injection molding, 30% glass fiber reinforced Recycled nylon 6.6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | ISO 527-2 |
Pasargad Polymer Peyvand Pasamid 3P-H1145B Nylon 6, 45% Glass Fiber Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | ISO 527 |
Grupo Repol Dinalon® B1S25 G30 PA6 30% Glass Fiber Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | d.a.m.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® BKV 130 GIT DUS008 900116 Nylon 6, Impact Modified PA 6, 30% glass fibers, injection molding, impact modified, GIT/WITInformation provided by LANXESS. |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | ISO 527-1,-2 |
Lanxess Pocan® B 3233 HR 000000 Polybutylene Terephthalate, 30% Glass Fibers PBT, 30% glass fibers, injection molding, improved flowability, hydrolysis stabilized |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | ISO 527-1/-2 |
Lanxess Durethan® BKV 30 H2.0 EF 900116 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, good flowability (Easy Flow), good heat-ageing resistance |
|||
Tensile Modulus | 9.03 GPa | 1310 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP DX06412H PC LNP* THERMOCOMP* DX06412H is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Tensile Modulus | 9.04 GPa | 1310 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP EXTC8143 PC (Asia Pacific) LNP* Thermocomp* EXTC8143 is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good ductility, No.. |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | Injection Molded; ASTM D638; ISO 527-2 |
Styron DLGF9411.00 Polypropylene Overview: DLGF 9400.00 is a 40% long glass fiber reinforced grade with good flow properties. The glass fibers (12 mm length) are coupled to the polypropylene matrix resulting in high stiffness and s.. |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp RFC16 PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RFC16 is a compound based on PA 66 resin containing Glass Fiber, Carbon Fiber. Added features include: Easy Molding.This data was supplied by SABIC-IP for the Europe-Africa-Middle.. |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GTX GTX230 PPE+PA66 (Europe-Africa-Middle East) |
|||
Tensile Modulus | 9.00 - 11.0 GPa | 1310 - 1600 ksi | ISO 527 |
Vyncolit 2530 W Novolac Phenolic Mineral and organic filled phenolic molding compound with excellent thermal properties.USES: Lamp sockets, special lamp holders, pan handles and knobs.Information provided by Vyncolit, a Sumitomo Ba.. |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® 2SV-30H black 9992 PA610-GF30 Product Description: GRILAMID XE 3976 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mate.. |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSGZ-30 PA666-GF30 Product description: Grilon TSGZ-30 is a heat stabilized, normal viscosity, and impact modified PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSGZ-30 has the following important p.. |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® FE270050 BK099 Nylon 66
(Unverified Data**) 30% Glass/Mineral Reinforced Polyamide 66Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide RFC16 PA66/6, Glass/Carbon Fiber Filled, Injection Molded RFC16 is a Glass Fiber and Carbon Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as STAR C PA66 C 303VY Z3)Information provided by Eurostar. |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam BFR460B1 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR460B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TRV-4X9 PAMACM12-GF40 Product description: Grilamid TRV-4X9 is an amorphous, cycloaliphatic polyamide with 40% glass fibre reinforcement. Grilamid TRV-4X9 characterises itself through the following features: Very low shr.. |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | dry; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 GF30 Polyamide 6 - Glass Fiber Reinforced 30% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | ISO 527-1/-2 |
DSM Stanyl® TS256F6 Nylon 46-30% Glass Reinforced (Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | dry; ISO 527-1/-2 |
DSM Stanyl® TW241F5 PA46-GF25 Heat Stabilized, 25% Glass Reinforced |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Rynite® GW520CS NC010 Polyethylene Terephthalate (PET) 20% Glass Reinforced Flame Retardant Polyethylene Terephthalate with Improved Glow Wire Performance Rynite GW520CS NC010 is a 20% glass fiber reinforced flame retardant color stabilized modified pol.. |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4192 black 9992 PA610-GF30 Information provided by EMS Grivory |