Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 8.65 GPa | 1250 ksi | STN EN ISO 527-2 |
Plastcom PLASTAMID® 6 GF 30 005 PA6 reinforced with glass fiber PA 6 for injection molding, reinforced with 30% glass fiber, used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools, hobby tools, gears, covers.. |
|||
Tensile Modulus | 8.62 GPa | 1250 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ PS-30GF/2S Natural Polybutylene Terephthalate (PBT) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Modulus | 8.62 GPa | 1250 ksi | ASTM D638 |
Solvay Specialty Polymers Veradel® AG-230 Polyethersulfone
(discontinued **) For superior long-term performance at high temperatures in severe service environments. It offers especially good toughness, hydrolytic stability, chemical resistance, plus FDA and USDA compliance.N.. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | ASTM D638 |
Plenco Valite 4224 Novolac Phenolic, Granular, Transfer Molded
(discontinued **) This Valite product has been replaced by Plenco 4224. Data provided by Plenco.VALITE 4224 is a brown, two stage, general purpose phenolic molding compound. It has good electrical and moldability ch.. |
|||
Tensile Modulus | 8.62 GPa | 1250 ksi | ASTM D638 |
Fiberfil® J-69/40/E High performance polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 8.62 GPa | 1250 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP EX07305 PEI (Asia Pacific) Polyetherimide reinforced with Glass fiber and PTFE for use in Burn-in Test Sockets (BiTS) Application |
|||
Tensile Modulus | 8.62 GPa | 1250 ksi | ASTM D638 |
Solvay Technyl® A20V25 25% Glass Filled, V-0 Nylon 66 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon DE002E PC (Europe-Africa-Middle East) LNP* STATKON* DE002E is a compound based on Polycarbonate resin containing Carbon Fiber. Added features include; Easy Molding.This data was supplied by SABIC-IP for the Europe-Africa-Middle East reg.. |
|||
Tensile Modulus | 8.62 GPa | 1250 ksi | ASTM D638 |
Solvay Specialty Polymers Veradel® AG-330 Polyethersulfone (PESU), 30% Glass Fiber Veradel® AG-330 is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, .. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON SE003 PA 12 (Europe-Africa-Middle East) LNP* Stat-kon* SE003 is a compound based on Nylon 12 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 8.61 GPa | 1250 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP KF004AL Acetal Homopoly (Asia Pacific) LNP* Thermocomp* KF004AL is a compound based on Acetal Homopolymer resin containing Glass Fiber. Added features of this material include: Low Extractible. |
|||
Tensile Modulus | 8.61 GPa | 1250 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP KF004AL Acetal Homopolymer LNP* THERMOCOMP* KF004AL is a compound based on Acetal Homopolymer resin containing 20% Glass Fiber. Added features of this material include: Low Extractible. |
|||
Tensile Modulus | 8.62 GPa | 1250 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP LF004E PEEK LNP* THERMOCOMP* LF004E is a compound based on Polyetheretherketone resin containing 20% Glass Fiber. Added features of this material include: Easy Molding. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RF005SXS PA 66 LNP THERMOCOMP* RF005SXS is a compound based on Nylon 66 resin containing 25% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Tensile Modulus | 8.63 GPa | 1250 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP DF006 PC LNP* Thermocomp* DF006 is a compound based on Polycarbonate resin containing 30% Glass Fiber. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | ASTM D638 |
Plenco 2308 Phenolic, Granular, Injection Molded PLENCO 02308 is a general purpose organic filled phenolic molding compound, offering improved heat resistance and optimized cure properties. UL recognized under component file E40654. 02308 is avai.. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN FR52G20NH NC010 Polyphthalamide (PPA)
(Unverified Data**) 20% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G20NH NC010 is a 20% glass reinforced flame retardant lubricated high performance polyamide resin. It.. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R525H BK0201 Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H BK0201 is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R525H Nylon 66, 25% Glass Filled, Dry as Molded Vydyne® R525H is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties whe.. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® S3 GF 30 1 (3222) PA 6.10 Dry, 30% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Tensile Modulus | 8.63 GPa | 1250 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36HL PC LNP LUBRICOMP* DFL36HL is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractable, Healthcare. |
|||
Tensile Modulus | 8.59 GPa | 1250 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON ME003S PP LNP* STAT-KON* ME003S is a compound based on Polypropylene resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Heat Stabilized. |