Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.855 GPa | 124 ksi | ASTM D638 |
Quadrant EPP TIVAR® 88 ESD UHMW-PE, Premium Glass Filled, Crosslinked Electro Static Dissipative Lining Material (ASTM Product Data Sheet) |
|||
Tensile Modulus | 0.854 GPa | 124 ksi | ISO 527 |
Gromax 1172LL TPE 1172LL is high modulus grade with nominal Durometer hardness of 72D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like blow molding grade. Charac.. |
|||
Tensile Modulus | 0.853 GPa | 124 ksi | |
Kuraray HYBRAR® HD3 Thermoplastic Rubber-HDPE Blend Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Tensile Modulus | 0.852 GPa | 124 ksi | Storage |
Epoxy Technology EPO-TEK® 730 General Purpose Epoxy Product Description: EPO-TEK® 730 is a two component, thixotropic, room temperature-curing epoxy adhesive. Advantages & Application Notes: Excellent all purpose adhesive. Many uses in job shop and .. |
|||
Tensile Modulus | 0.853 GPa @Temperature 30.0 °C |
124 ksi @Temperature 86.0 °F |
50%RH; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 101F NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101F NC010 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont .. |