Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.800 GPa | 116 ksi | ISO 527-1 |
Polikim ULPOLEN® 1000 UHMWPE, Flame Retardant For those producing flammable materials and in the mining industry, explosion and fire are major dangers. It is of vital importance that in conveyor belts and bunkers, lining material is flame retar.. |
|||
Tensile Modulus | 0.800 GPa | 116 ksi | ASTM D638 |
Quadrant EPP TIVAR® 1000 UV Stabilized UHMW, Black (ASTM Product Data Sheet) |
|||
Tensile Modulus | 0.800 GPa | 116 ksi | ASTM D638 |
Quadrant EPP TIVAR® 1000 UV Stabilized UHMW-PE, Natural & Colored Except Black (ASTM Product Data Sheet) |
|||
Tensile Modulus | 0.800 GPa | 116 ksi | Secant; ASTM D638 |
NOVA Chemicals Novapol® HD-2100-U MDPE Extrusion Resin Features: Excellent ESCR and toughness, high strength, excellent processability.Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.Data provided by the manufacturer. |
|||
Tensile Modulus | 0.800 GPa | 116 ksi | Secant; ASTM D638 |
NOVA Chemicals Novapol® HD-2100-A MDPE Extrusion Resin
(discontinued **) Features: Excellent ESCR and toughness, high strength, excellent processability.Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.Data provided by the manufacturer. |
|||
Tensile Modulus | 0.800 GPa | 116 ksi | 1 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 2-3302 TO BU Elastomer Modified, UV-Stabilized Polypropylene Block-Copolymer INNOPOL® CS 2-3302 TO BU is an elastomer modified, UV-stabilized compound based on polypropylene block-copolymer.INNOPOL® CS 2-3302 TO BU is developed for producing injection molded automotive.. |
|||
Tensile Modulus | 0.800 GPa | 116 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® B 35 FKA 000000 Nylon 6, Film Grade PA 6 Film grade, medium viscosity, nucleated, with processing and slip additives, in compliance with FDA for food contactApplication Examples: flat and blown film, flat film coextrusion for PA/PE co.. |
|||
Tensile Modulus | 0.800 GPa | 116 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® B 40 F 000000 Nylon 6, Film Grade PA 6, Film grade, high viscosity, without additives or processing aids, in compliance with FDA for food contact and acc. the German BgVV Recommendation XLIV, Section VI.A" Synthetic casings in polya.. |
|||
Tensile Modulus | 0.800 GPa | 116 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® B 40 FAM 000000 Nylon 6, Film Grade PA 6 film grade of high viscosity with high slip agent and lubricant content, not nucleatedApplication Examples: flat and blown film with good surface slip and smoothness - including in the freshly .. |
|||
Tensile Modulus | 0.800 GPa | 116 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® BC 304 H3.0 000000 Nylon 6 PA 6, injection molding grade, non-reinforced, elastomer-modified, extremely high notched impact strength, including in the dry state and at low temperatures, also applicable for barrier layers in e.. |
|||
Tensile Modulus | 0.800 - 1.20 GPa | 116 - 174 ksi | DIN 53457 |
Isoflon PVDF Polyvinyl Dichloride Fluoropolymer Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Tensile Modulus | 0.800 GPa | 116 ksi | ISO 527 Type 1A |
Solvay TECHNYL® eXten D 458P PA6.10, DRY Description: Product in development - provisional datasheet. High viscosity unfilled plasticized PA6.10 for extrusion applications providing low end part warpage.Available in: Asia Pacific, Europe, .. |
|||
Tensile Modulus | 0.800 GPa | 116 ksi | At 1 mm/min; ISO 527-2 |
Borealis Borcoat™ BB125E Polypropylene Adhesive for Steel Pipe Coating Borcoat BB125E is a chemically modified polypropylene copolymer designed to be used as the tie layer between the epoxy corrosion protection layer and the top-coat polypropylene Borcoat BB108E-1199.B.. |
|||
Tensile Modulus | 0.800 GPa | 116 ksi | At 1 mm/min; ISO 527-2 |
Borealis Borstar® ME3440 Black Medium Density Polyethylene for Pressure Pipes Borstar ME3440 is a black, bimodal medium density polyethylene compound classified as a MRS 8.0 material (PE80), with optimum balance between flexibility and strength, produced with the advanced Bor.. |
|||
Tensile Modulus | 0.800 GPa | 116 ksi | DIN EN ISO 527 |
Wolf Kunststoff ZEDEX® ZX-550 A5L Polymer Alloy Main Characteristics: Strong anti-adhesive; Low creep; Weather resistant; No water absorption; Good machinability; Strongly viscoelastic; Stress resistantApplications: Chemical Engineering; Laborato.. |
|||
Tensile Modulus | 0.800 GPa | 116 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® EB 50 H PA6 Product description: Grilon EB 50 H is a high viscosity, unreinforced, heat stabilized PA6 extrusion blow mounding grade. Grilon EB 50 H has the following important properties: High melt strengthImp.. |
|||
Tensile Modulus | 0.800 GPa @Temperature 120 °C |
116 ksi @Temperature 248 °F |
ISO 527-1/-2 |
DSM Stanyl® TS300 PA46 |
|||
Tensile Modulus | 0.800 GPa | 116 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4181 black PA1010 Product description: Grilamid XE 4181 black 9992 is a unreinforced, high viscosity, plasticized, high impact resistant polyamide 1010 (PA1010) extrusion grade. Grilamid XE 4181 black 9992 is highly .. |
|||
Tensile Modulus | 0.800 GPa @Temperature 40.0 °C |
116 ksi @Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® ST820 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Polybutylene Terephthalate with Excellent Impact Resistance Crastin ST820 NC010 is an unreinforced Super Tough polybutylene terephthalate resin for injection molding.Information provide.. |
|||
Tensile Modulus | 0.800 GPa | 116 ksi | 1 mm/min |
Arkema Group Orgalloy® LE 60XV Flexible Nylon Alloy (Conditioned) LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents).Suited to the extrusion of tubes (hydraulic, pneumatic, painting..... |
|||
Tensile Modulus | 0.800 - 0.900 GPa | 116 - 131 ksi | |
Addcomp PRIEX® Ionomer 48101 PP random copolymer Ionomers will be used toStrengthen rigidity and hardness while maintaining impact resistance in polyolefinsMaintain adhesion even under contaminated conditions especially in fatty substratesReduce t.. |
|||
Tensile Modulus | 0.800 GPa | 116 ksi | |
BASF Novolen® 2800 J Polypropylene Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 0.800 GPa | 116 ksi | ASTM D638 |
Aclo Accuguard Polypropylene CP0467V0CSV Copolymer Flame Retardant Automotive Approved grade |
|||
Tensile Modulus | 0.800 GPa | 116 ksi | ASTM D638 |
Asahi Glass Fluon® ETFE A thermoplastic fluoropolymer developed by Asahi Glass. It is a copolymer comprising of tetrafluoroethylene and ethylene. Fluon® ETFE is a balanced fluoropolymer that has chemical resistance and el.. |
|||
Tensile Modulus | 0.800 GPa | 116 ksi | ISO 527-2 |
CENTROPLAST CENTROLEN PE-UHMW Ultra-high molecular weight polyethylene This plastic is a low density, easily machined material that can be welded and has a low sliding friction with high impact resistance. Applications include glide strips, pump components, and wearin.. |
|||
Tensile Modulus | 0.800 GPa | 116 ksi | |
LATI Latiohm 52/11-10 PD02 PP Homopolymer Dissipative product based on Polypropylene homopolymer (PPh). Unfilled.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Tensile Modulus | 0.800 GPa | 116 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® RS 3261THSL BK041A Nylon 610
(Unverified Data**) Toughened Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3261THSL BK041A is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient.. |
|||
Tensile Modulus | 0.800 GPa | 116 ksi | ISO 527-2 |
Borealis Borstar® ME3444 Blue Medium Density Polyethylene for Drinking Water Pipes Borstar 3444 is a blue, bimodal, medium density polyethylene classified as a MRS 8.0 material (PE80) produced with the advanced Borstar technology. A combination of pigments and stabilizers is incl.. |