Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.30 GPa | 1060 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp DCL329XZ PC LNP LUBRICOMP* DCL329XZ is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was sup.. |
|||
Tensile Modulus | 7.28 GPa | 1060 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36G PC LNP* Lubricomp* DFL36G is a compound based on Polycarbonate resin containing 30% Mixed Glass, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | ISO 527-1/-2 |
DSM Arnite® CCT GF20 (T-X01415) PBT-20% Glass Reinforced (European Grade)
(discontinued **) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Tensile Modulus | 7.30 GPa @Temperature 23.0 °C |
1060 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® LW9320LM BK591 PBT
(Unverified Data**) Crastin® LW9320LM is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. It has excellent surface aspect, dimensional stability and low warpage and was developed fo.. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | ASTM D638 |
Solvay Specialty Polymers Radel® R-7120 Polyphenylsulfone, 20% glass fiber
(discontinued **) RADEL R 7120 is a 20% glass fiber reinforced grade of RADEL R polyphenylsulfone developed specifically for aircraft interior applications. The product complies with the FAA regulation 14CFR Part 25 .. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | ISO 527-1/-2 |
Lanxess Durethan® DP 2131/20 H2.0 900051 Nylon 6, 20% Glass Fiber PA 6, injection molding grade, 20% glass fibers, better surface resistance to alcoholic calcium chloride-solution than BKV 20 H2.0, good heat-ageing resistance and weather resistance |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | 1 mm/min; ISO 527-1,-2 |
Gromax BFG30-DN00N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Modulus | 7.31 GPa @Temperature 100 °C |
1060 ksi @Temperature 212 °F |
4; ISO 527-2 |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Dry) Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high stre.. |
|||
Tensile Modulus | 7.31 GPa @Temperature 150 °C |
1060 ksi @Temperature 302 °F |
4; ISO 527-2 |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica.. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DEL329XF PC LNP STAT-KON* DEL329XF is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 15% PTFE. Added features include: Electrically Conductive. Wear Resistant, Flame Retardant. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DEL329XF PC (Asia Pacific) LNP STAT-KON* DEL329XF is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 7.28 GPa | 1060 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP JF004LZ PES LNP* Thermocomp* JF004LZ is a compound based on PES containing 20% Glass Fiber. Added features include: Extrusion Grade, Low Extractible. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RF004 PA 66 LNP THERMOCOMP* RF004 is a compound based on Nylon 66 resin containing 20% Glass Fiber. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RF004H PA 66 LNP* THERMOCOMP* RF004H is a compound based on Nylon 66 containing 20% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RF004XXD PA 66 LNP THERMOCOMP* RF004XXD is a compound based on Nylon 66 resin containing 20% Glass Fiber. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | 1 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 226F4 Nylon 6.6, 20% Glass Fiber SAXAMID 226F4 is a polyamide 6.6 injection-molding-grade reinforced with 20% glass fibers.Information provided by SAX Polymers |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl GFN1430V PPE+PS Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable.. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GTX GTX830 PPE+PA (Europe-Africa-Middle East) NORYL GTX830 a 30% glass reinforced grade which offers an excellent combination of chemical/heat resistance in combination with stiffness. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl GFN1430V PPE+PS (Asia Pacific) Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable.. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | ISO 527-1/-2 |
Unitika BV2120G15 PA66, 15% Glass Fiber Reinforced, Flame Retardant, Dry Information provided by Unitika Ltd. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® LW9320LM BK591 PBT+SAN
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9320LM is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. It ha.. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | 1 mm/min; ISO 527 |
Eurostar Star X 1615 33V S4 PA66, Glass Fiber Reinforced, UV stabilized, Injection Molding Star X 1615 33V S4 is an Impact Modified, Glass Fiber Reinforced, UV stabilized Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | ISO 527-1 |
Barlog Plastics KEBAFORM C 2527 POM Copolymer, 25% glass fiber reinforced POM-GF25Information provided by BARLOG plastics GmbH. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® B3 GF 35 (2473) PA 6 Conditioned, 35% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | Elasticity; ISO 527-2 |
BASF Ultrason E 2010 G4 20% Glass Filled PES Ultrason E 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength. |
|||
Tensile Modulus | 7.28 GPa | 1060 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36G PC (Asia Pacific) LNP* Lubricomp* DFL36G is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Milled Glass. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 7.31 GPa @Temperature 150 °C |
1060 ksi @Temperature 302 °F |
ISO 527-2 |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically .. |