Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.20 GPa | 1040 ksi | |
Plastcom SLOVASTER® B/A GF 20 PBT, 20% glass fibre FeaturesPBT/ASA for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and ben.. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | ISO 527 |
Nilit FRIANYL A63 HS-GV30 Nylon 6.6 for injection molding, 30% glass fiber reinforced Nylon 6.6 for injection molding, high impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | |
Radici Radilon® S RV200 (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | |
Radici Radilon® S RV330 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | ISO 527-2/1A |
Radici Raditer® B RV 200 Polybutylene Terephthalate with 20% Glass fiber Raditer® B RV 200 is a glass fiber reinforced thermoplastic polyester based on polybutylene terephthalate. The PBT compounds combine excellent thermal, mechanical, electrical and chemical properti.. |
|||
Tensile Modulus | 7.19 GPa | 1040 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DFL34EH PC LNP* LUBRICOMP* DFL34EH is a compound based on Polycarbonate containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Easy Molding, Healthcare, Wear Resistant. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | 1 mm/min; ISO 527-1,-2 |
Gromax BFG30-EN03N1 Nylon 6 33% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Modulus | 7.14 GPa | 1040 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP EX06405 PEI LNP* LUBRICOMP* EX06405 is a compound based on Polyetherimide resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible, Easy Molding. |
|||
Tensile Modulus | 7.14 GPa | 1040 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP EX06405 PEI (Asia Pacific) LNP* Lubricomp* EX06405 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM CRS5201R PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. Resin is RoHS com.. |
|||
Tensile Modulus | 7.17 GPa | 1040 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DEL329XF PC (Asia Pacific) LNP STAT-KON* DEL329XF is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 7.14 GPa | 1040 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp KF003 Acetal Copoly LNP* Thermocomp* KF003 is a compound based on Acetal Copolymer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 7.18 GPa | 1040 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp RF004S PA 66 LNP* Thermocomp* RF004S is a Nylon 6/6 containing Glass Fiber. Characteristics are Heat Stabilized.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 7.15 GPa | 1040 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp OF002A PPS LNP* Thermocomp* OF002A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 7.15 GPa | 1040 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp OF002A PPS (Asia Pacific) LNP* Thermocomp* OF002A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 7.17 GPa | 1040 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL FE1520PW PPE+PS (Europe-Africa-Middle East) Noryl* FE1520PW resin is a blend of polyphenylene oxide (PPO) and polystyrene (PS) resin that contains 20% glass reinforcement. The resin is suitable for injection molding. Noryl FE1520PW resin has .. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | ISO 527-1/-2 |
DSM Akulon® F249-HG4 Nylon 6-20% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 GV 35 HWCP 35% Glass Fiber Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-2H black PA*-GF20 Product description: Grivory GV-2H is a 20% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide. Grivory.. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4174 black 9992 PA1010-GF30 Product description: Grilamid XE 4174 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 1010 injection molding grade. The main features of Grilamid XE 4174 black 9992 are: PA1010.. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 70G30HSLR BK099 Nylon 66
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G30HSLR BK099 is a 30% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection mol.. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 70G30L NC010 Nylon 66
(Unverified Data**) 30% Glass Reinforced Polyamide 66Zytel 70G30L NC010 is a 30% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide RFB53U PA66, 50% Glass Bead/Fiber Filled, Injection Molded RFB53U is a Glass Bead/ Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 1525 VK Z4)Information provided by Eurostar. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-2 FWA black 9225 PA*-GF20 Product description: Grivory GV-2 FWA black 9225 is a 20% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copoly.. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | ISO 527-1/-2 |
BASF Ultramid® B3EG7 35% Glass Filled PA6 (Conditioned) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |