Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.0131 - 0.0145 GPa | 1.90 - 2.10 ksi | |
Bulk Molding Compounds BMC 850 Corrosion Resistant, Flame Retardant Molding Compound BMC 850 is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications a.. |
|||
Tensile Modulus | 0.0131 - 0.0145 GPa | 1.90 - 2.10 ksi | |
Bulk Molding Compounds BMC 851 Corrosion Resistant, Flame Retardant Molding Compound BMC 851is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications ar.. |