Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.00827 GPa | 1.20 ksi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable W2402L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Modulus | 0.00827 GPa | 1.20 ksi | Type IV, 510 mm/min; ASTM D638 |
PolyOne FireCon™ CPE 30-11 REV 2 Polyethylene, Chlorinated (CPE) CPE-30-11 REV 2 is a heavy duty thermoplastic jacket for power and control cables. It is suitable for VW1 and tray fire rated applications. CPE-30-11 REV 2 offers high tensile and superior fluid res.. |
|||
Tensile Modulus | 0.00827 GPa | 1.20 ksi | Type IV, 510 mm/min; ASTM D638 |
PolyOne FireCon™ CPE 30-11 RoHS BLACK Polyethylene, Chlorinated (CPE) CPE-30-11 RoHS BLACK is a heavy duty thermoplastic jacket for power and control cables. It is suitable for VW1 and tray fire rated applications. CPE-30-11 RoHS BLACK offers high tensile and superior.. |
|||
Tensile Modulus | 0.00827 GPa | 1.20 ksi | Type IV, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV 1144 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Tensile Modulus | 0.00827 GPa | 1.20 ksi | ASTM D1708 |
DuPont Elvax® 4320 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 4320 is an ethylene-vinyl acetate / acid terpolymer resin for use in industrial applications.ApplicationsElvax® 4320 resins can be used for the following applications: adhesives, s.. |
|||
Tensile Modulus | 0.00827 GPa | 1.20 ksi | (0.2 in/min), Molded Properties; ASTM D638 |
ExxonMobil Escorene™ MV 02528EH2 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 02528EH2 is a copolymer of ethylene and vinyl acetate.Availability: Asia Pacific and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Free Flowing Agent: Yes A.. |
|||
Tensile Modulus | 0.00827 GPa | 1.20 ksi | (0.2 in/min), Molded Properties; ASTM D638 |
ExxonMobil Escorene™ UL 02133EN2 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 02133EN12 is a copolymer of ethylene and vinyl acetateAvailability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: NoFree Flowing Agent:.. |
|||
Tensile Modulus | 0.00827 GPa | 1.20 ksi | ASTM D638 |
ExxonMobil Escorene™ UL 04331EL Ethylene Vinyl Acetate Copolymer Product Description: UL 04331EL is a HEVA grade, especially designed for photovoltaic cells and encapsulation applications, requiring a good balance of adhesion and COF. It offers excellent light tr.. |
|||
Tensile Modulus | 0.00827 GPa | 1.20 ksi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable WC9000L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |