Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.00345 GPa | 0.500 ksi | Type IV, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV 3716 Polyvinyl Chloride, Flexible (PVC, Flexible) A Filled PVC compound formulated specifically for FDA extrusion and Molding applications.The physical properties listed below, are typical values obtained on compression molded sheets and tested in .. |