Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.000138 GPa | 0.0200 ksi | ASTM D3574 |
Saint-Gobain Korel® K20 Very Soft Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® mi.. |