Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 8.50 - 10.0 GPa | 1230 - 1450 ksi | ISO 527 |
Vyncolit 4451 XB Novolac Phenolic Organic and mineral filled phenolic molding compound with excellent mechanical properties (highest notched impact strength).USES: Fuse holders, brush holders, circuit breakers, automotive ignition a.. |