Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.500 - 0.600 GPa | 72.5 - 87.0 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Hyflon® PFA 120 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Tensile Modulus | 0.500 - 0.600 GPa | 72.5 - 87.0 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Hyflon® PFA 125 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Tensile Modulus | 0.500 - 0.600 GPa | 72.5 - 87.0 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Hyflon® PFA 420 Perfluoroalkoxy (PFA) Hyflon® PFA is a family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resistance.. |
|||
Tensile Modulus | 0.500 - 0.600 GPa | 72.5 - 87.0 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Hyflon® PFA M620 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Tensile Modulus | 0.500 - 0.600 GPa | 72.5 - 87.0 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Tensile Modulus | 0.500 - 0.600 GPa | 72.5 - 87.0 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Tensile Modulus | 0.500 - 0.600 GPa | 72.5 - 87.0 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Hyflon® PFA P455 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Tensile Modulus | 0.400 - 0.600 GPa | 58.0 - 87.0 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF) Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional .. |
|||
Tensile Modulus | 0.500 - 0.600 GPa | 72.5 - 87.0 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Hyflon® MFA® 1041 Perfluoropolymer Hyflon® MFA 1041 is a high extrusion speed resin specifically designed for insulation for plenum-rated LAN cables. MFA 1041 delivers superior electrical performance in addition to its excellent f.. |
|||
Tensile Modulus | 0.500 - 0.600 GPa | 72.5 - 87.0 ksi | MD/TD; ISO 527-3 |
Borealis BA11CF Polypropylene Copolymer BA110CF is a heterophasic copolymer. This grade is suitable for use on chill roll processes. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. .. |
|||
Tensile Modulus | 0.500 - 0.600 GPa | 72.5 - 87.0 ksi | MD/TD; ISO 527-2 |
Borealis BB213CF Polypropylene Copolymer BB213CF is a heterophasic copolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: BB213CF is recommended for food packaging.. |
|||
Tensile Modulus | 0.500 - 0.600 GPa | 72.5 - 87.0 ksi | MD/TD; ISO 527-3 |
Borealis BorPure™ RD234CF Polypropylene Random Copolymer BorPure™ RD234CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD234CF is recommended for food packaging, stationa.. |
|||
Tensile Modulus | 0.500 - 0.600 GPa | 72.5 - 87.0 ksi | MD/TD; ISO 527-3 |
Borealis RD204CF Polypropylene Random Copolymer RD204CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD204CF is recommended for blending, food packaging, high qua.. |
|||
Tensile Modulus | 0.500 - 0.600 GPa | 72.5 - 87.0 ksi | MD/TD; ISO 527-3 |
Borealis RD461CF Polypropylene Random Copolymer RD461CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD461CF is recommended for food packaging, high quality stati.. |
|||
Tensile Modulus | 0.500 - 0.600 GPa | 72.5 - 87.0 ksi | MD/TD; ISO 527-3 |
Borealis RD734CF Polypropylene Random Copolymer RD734CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD734CF is recommended for food packaging, high quality stati.. |
|||
Tensile Modulus | 0.500 - 0.600 GPa @Temperature 23.0 °C |
72.5 - 87.0 ksi @Temperature 73.4 °F |
1.0 mm/min; ASTM D1708 |
Solvay Specialty Polymers Hyflon® PFA 420 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon® PFA is a family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resistance, .. |
|||
Tensile Modulus | 0.500 - 0.600 GPa @Temperature 23.0 °C |
72.5 - 87.0 ksi @Temperature 73.4 °F |
1.0 mm/min; ASTM D1708 |
Solvay Specialty Polymers Hyflon® PFA M620 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |
|||
Tensile Modulus | 0.500 - 0.600 GPa @Temperature 23.0 °C |
72.5 - 87.0 ksi @Temperature 73.4 °F |
1.0 mm/min; ASTM D1708 |
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |
|||
Tensile Modulus | 0.500 - 0.600 GPa @Temperature 23.0 °C |
72.5 - 87.0 ksi @Temperature 73.4 °F |
1.0 mm/min; ASTM D1708 |
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |
|||
Tensile Modulus | 0.400 - 0.600 GPa @Thickness 2.00 mm, Temperature 23.0 °C |
58.0 - 87.0 ksi @Thickness 0.0787 in, Temperature 73.4 °F |
Type IV, 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Information provided by Solvay Specialty Polymers. |