Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.80 GPa | 1420 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID® 6 GF 30 AS PA6 reinforced with glass fiber, anti-static agent PA 6 for injection molding, reinforced with 30% glass fiber, contains antistatic agent for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric.. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | ISO 527-1/-2 |
DSM Akulon® S223-HPG8U (Dry) 43% Glass Reinforced, Impact Modified Nylon 66 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 1 mm/min; ISO 527-1,-2 |
Gromax BFG30-FH00N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | ISO 527-1/-2 |
Lanxess Durethan® BKV 30 000000 Nylon 6, 30% Glass Fiber 30% Glass fiber reinforced; injection molding grade |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | ISO 527-1/-2 |
Lanxess Pocan® B 4235 Z 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant, impact modified |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 1 mm/min; ISO 527-1,-2 |
Lanxess Pocan® BF 4232 HR 901510 PBT, 30% Glass Fiber PBT, 30% glass fiber, injection molding, flame retardant, hydrolysis stabilizedInformation provided by LANXESS. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | ISO 527 Type 1A |
Solvay TECHNYL® B 218 V30 Black 21 N PA66, 30% glass fiber, DRY Description: Copolyamide PA66/6, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHNYL® B 218 V30 is used i.. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36XXY PA 66 LNP* LUBRICOMP* RFL36XXY is a compound based on Nylon 66 containing 30% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RFP36 PA 66 LNP* LUBRICOMP* RFP36 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE, Silicone. Added features of this material include: Wear Resistant. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RFP36S PA 66 LNP* LUBRICOMP* RFP36S is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 2412EPR PEI (Asia Pacific) 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the As.. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 2412EPR PEI (Europe-Africa-Middle East) 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu.. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON MV007SU PP (Europe-Africa-Middle East) LNP* VERTON * MV007SU is a compound based on PP resin containing Long Glass Fiber. Added features include; Chemically Coupled, Heat Stabilized, UV Stabilizedl. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON MV007SUP PP (Europe-Africa-Middle East) LNP* VERTON* MV007SUP is a compound based on PP resin containing Long Glass Fiber. Added features include; Chemically Coupled, Heat Stabilized, UV Stabilized. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON MV007U PP (Europe-Africa-Middle East) LNP* VERTON* MV007U is a compound based on PP resin containing Long Glass Fiber. Added features include; Chemically Coupled, Heat Stabilized, UV Stabilized. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 1 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 226F6 Nylon 6.6, 30% Glass Fiber SAXAMID 226F6 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers. It has very high mechanical strength in combination with good flow properties. It shows hig.. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP QFL36 PA 6/10 LNP LUBRICOMP* QFL36 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | ASTM D638 |
Plenco 3303 Phenolic, Granular, Injection Molded Plenco 03303 is a renumber of Plaslok 5303. Plenco 03303 is a two-stage, mineral and flock-filled phenolic molding compound offering excellent electrical insulating properties. It can be processed b.. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | ASTM D638 |
Plenco 4349 Phenolic, Granular, Compression Molded PLENCO 04349 is a heat resistant, mineral filled phenolic molding compound offering optimized cure characteristics, and excellent heat resistant properties. PLENCO 04349 is also formulated to offer .. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | ASTM-D790 |
Polyram PlusTek PA309G6 Nylon 6.6, 30% Glass Fiber 30% glass fiber reinforced, UV stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | ISO 527 |
Polyram RamLloy PFS301G6 ASA/PBT Alloy, 30% Glass Fiber 30% Glass fiber reinforced ASA/PBT alloy for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | dry; ISO 527-1/-2 |
DSM Novamid® 1015G33-8 NAT PA6-GF33 33% Glass Reinforced, Injection Molding |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® LW9330 NC010 PBT+SAN
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9330 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. I.. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 70G30L NC010 Nylon 66
(Unverified Data**) 30% Glass Reinforced Polyamide 66Zytel 70G30L NC010 is a 30% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G30HSL BK416 is a 30% glass fiber reinforced heat stabilized lubricated black polyamide 6 resin for injection molding.Information provided by.. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® FE5382 BK276 Nylon 612
(Unverified Data**) 33% Glass Reinforced Polyamide 612 Developed for Electrical and Electronics Applications Zytel FE5382 BK276 is a 33% glass fiber reinforced heat stabilized black polyamide 612 resin developed for el.. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | ISO 527-1/-2 |
BASF Ultradur® B 4300 G6 FC 30% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | ISO 527-1/-2 |
BASF Ultradur® B 4300 G6 LT 30% Glass Filled BK 150926 PBT Description: Easy flowing injection molding grade with 30 % glass fibers; for rigid, tough and dimensionally stable technical parts (eg windshield wiper arms, printed circuit boards PCBs), housing, .. |