Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.76 GPa | 1420 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Verton NV0061EV_GY7E148 PC+ABS Preliminary data for 30% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region. |