Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.65 GPa | 1400 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne OnForce™ LFT UR-30 LGF/000 Natural Polyurethane, Unspecified (PUR, Unspecified) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Tensile Modulus | 9.65 GPa | 1400 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ 81530 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 9.65 GPa | 1400 ksi | ASTM Data |
Dow Questra® EA503 High Heat Syndiotactic Polystyrene, 30% Glass Filled
(discontinued **) QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve.. |
|||
Tensile Modulus | 9.65 GPa | 1400 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36ELH PC (Asia Pacific) LNP* Lubricomp* DFL36ELH is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Tensile Modulus | 9.65 GPa | 1400 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DE0039 PC LNP* STAT-KON* DE0039 is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Flame Retardant. Electrically Conductive. |
|||
Tensile Modulus | 9.65 GPa | 1400 ksi | 45° stress angle |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Unidirectional CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |
|||
Tensile Modulus | 9.65 GPa | 1400 ksi | 90° stress angle |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Unidirectional CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |
|||
Tensile Modulus | 9.65 GPa | 1400 ksi | ASTM D638 |
Ensinger Tecatron® XP-81 Compression Molded PPS Compound, Filled with 15% Graphite and 15% Carbon Fiber Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Tensile Modulus | 9.65 GPa | 1400 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AT-30GF/000 Acetal-Copolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |