Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.16 GPa | 1330 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DE0021E PC LNP STAT-KON* DE0021E is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding, Flame Retardant, Electrically Conductive. |
|||
Tensile Modulus | 9.16 GPa | 1330 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DE0021E PC (Asia Pacific) LNP STAT-KON* DE0021E is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Easy Molding. |
|||
Tensile Modulus | 9.16 GPa | 1330 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Verton PV007SV_WH8D537 PA 6 Preliminary data for 35% long fiber single pellet color filled PA6This data was supplied by SABIC-IP for the Americas region. |