Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.10 GPa | 1320 ksi | |
Radici Radiflam® A RV300AF (dry) Nylon 66-30GF Radiflam® A is a range of flame retardant polyamides 66 (PA 66) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici g.. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® A-4122 HR WH 117 Polyphthalamide (PPA)
(Unverified Data**) Amodel A-4122 HR resin is a 22% glass reinforced polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhibits high heat resistance, high st.. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® A-4122 LS WH678 Polyphthalamide (PPA)
(Unverified Data**) Amodel A-4122 LS is a 22% glass fiber reinforced, light-stabilized, high-reflectivity white grade of Amodel polyphthalamide (PPA). It is designed to provide high crystallinity when molded in water-c.. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® A-4422 LS WH118 Polyphthalamide (PPA)
(Unverified Data**) Amodel A-4422 LS resin is a 22% reinforced, light-stabilized, high-reflectivity white grade of polyphthalamide (PPA). The material exhibits high heat resistance, high strength and stiffness over a b.. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | |
Idemitsu Kosan Xarec® WA 552 SPS, 30% Glass Filled Crystalline Polymer, Glass Filled/Impact Modified. Used in Automotive and Industrial applications. NSF and medical approval ISO 10993 |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218 V35 Black 21NHFE PA66, 35% glass fiber, Conditioned Description: TECHNYL® A 218 V35 BLACK 21NHFE is polyamide 6.6, high flow, reinforced with 35% glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefit.. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® A-4122 HR WH 117 Polyphthalamide (PPA), 22% Glass Fiber Amodel® A-4122 HR resin is a 22% glass reinforced polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhibits high heat resistance, hig.. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP DF006 PC (Asia Pacific) LNP* Thermocomp* DF006 is a compound based on Polycarbonate resin containing Glass Fiber. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP DF0069P PC LNP THERMOCOMP* DF0069P is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Exceptional Processing. Flame Retardant. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RF005SXS PA 66 LNP THERMOCOMP* RF005SXS is a compound based on Nylon 66 resin containing 25% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | ASTM D638 |
Plenco 4304 Phenolic, Nodular, Transfer Molded PLENCO 04304 is a heat resistant, mineral filled phenolic molding compound offering improved mechanical strength properties along with excellent dimensional stability. UL recognized under component .. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | ASTM D638 |
Plenco 7500 Phenolic, Granular, Compression Molded PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi.. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | ISO 527 |
Polyram RamSter PF310G6 PBT Alloy, 30% Glass Fiber, UV Stabilized 30% Glass fiber reinforced PBT alloy, low warp properties, UV stabilized for injection molding.Information provided by Polyram. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | Longitudinal |
Goodfellow Polyethylene Fiber/Polyethylene composite Information provided by Goodfellow. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | ASTM D638 |
Plenco 4311 Phenolic, Granular, Injection Molded PLENCO 04311 is a heat resistant, mineral filled phenolic molding compound offering excellent processability, mechanical strength, and improved cold powder pourability characteristics. UL recognized.. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | ASTM D638 |
Ecomass® 1050CO94 Copper Filled Polyamide Nontoxic alternative to Lead (Pb), weighting and balancing applicationsModerate Specific GravityCopper Powder Filled Polyamide (PA) AlloyGood ToughnessInformation provided by Technical Polymers |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | ASTM D638 |
Ecomass® 1080CO94 Copper Powder Filled Polyamide Alloy, Injection Molding Moderate Specific Gravity, Copper Powder Filled Polyamide (PA) Alloy, Good Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting and balancing.. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | dry; ISO 527-1/-2 |
DSM Novamid® 1010G30 NA PA6-GF30 30% Glass Reinforced, Injection Molding, Easy Molding Grade, High Flow |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam RF0059 PA66, Glass Fiber, Flame Retardant, Injection Molded Starflam RF0059 is a Flame Retardant, Glass Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam AFR450B1 PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR450B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 909 BK Nylon 66/6, 25% Glass Reinforced, DAM Vydyne® 909 BK is a halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwrite.. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6
(Unverified Data**) 30% Glass Reinforced Toughened Polyamide 6 Zytel 73G30T NC010 is a 30% glass fiber reinforced toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 909 Nylon 66/6, 25% Glass Reinforced, Ignition Resistant, DAM Vydyne® 909 is halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwriters.. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | 1mm/min; ISO 527 |
BASF Ultramid® 8333G HI HS BK-102 33% Glass Filled PA6 (Dry) Ultramid 8333G HI HS BK-102 is a 33% glass reinforced, heat stabilized, impact modified, pigmented black, PA6 injection molding compound developed for applications requiring improved dry as molded t.. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | |
LATI Latimass 62-01 D025 PA6 Specific density compound based on Polyamide 6 (PA6). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter.. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® A-1422 LS WH 171 Polyphthalamide (PPA)
(discontinued **) Amodel A-1422 LS is a light-stabilized, high-reflectivity, 22%-reinforced white polyphthalamide (PPA) that exhibits high heat resistance, high strength and stiffness over a broad temperature range, .. |