Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.00 GPa | 1310 ksi | ASTM D638 |
Premix Premi-Glas® 2206-22 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2206-22 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | ASTM D638 |
Premix Premi-Ject® 1102H Fiberglass Reinforced Thermoset BMC Premi-Ject® 1102H is a fiberglass reinforced thermoset bulk molding compound for coil encapsulation applications.Key features and benefits are:Designed with unique flow properties to encapsulate co.. |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | ISO 527, ASTM D638 |
Nilit Nilamid A G5 FR PH1 25% Glass Fiber Reinforced, Flame Retardant PA66 Description: Nilamid A G5 FR PH1 combines flame retardancy with outstanding mechanical performance. This product has a complete yellow card, with RTI and CTI listings. The formulation has been optim.. |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | ISO 527-2/1A |
Radici Raditer® B RVA 300 Polybutylene Terephthalate with 30% Glass fiber Raditer® B RVA is a range of glass fiber reinforced Polybutylene terephthalate blends for injection molding, with excellent dimensional stability, low warpage and good surface aspect.Information pr.. |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | ISO 527 |
Nilit FRIANYL C73 GV30 Nylon 6.6/6 for injection molding, 30% glass fiber reinforced Nylon 6.6/6 for injection molding, medium viscosity.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | ISO 527 |
Nilit RECONYL A GV30 Recycled nylon 6.6 for injection molding, 30% glass fiber reinforced Recycled nylon 6.6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | ISO 527-2 |
Pasargad Polymer Peyvand Pasamid 3P-H1130W Nylon 6, 30% Glass Fiber Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | ISO 527-1/-2 |
Lanxess Pocan® DP 4035 000000 PBT + PET, 30% Glass Fiber PBT+PET, 30% glass fibers, injection molding, halogen free flame retardant |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | 1 mm/min; ISO 527-1,-2 |
Lanxess Pocan® KU 2-7241 000000 PBT, 25% Glass Fiber PBT, 25% glass fibers, injection molding, flame retardant, improved impact strengthInformation provided by LANXESS. |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 508 PBT (Europe-Africa-Middle East) VALOX 508 is a 30% glass reinforced PBT+PC blend with good warpage characteristics. Applications: appliance handles, spotlights, electric motors, distributor caps, ignition rotors, voltage regulator.. |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 830F PBT+PET PBT+PET, 30% Glass, Mold Release, Heat Stabilized, For food contact applications |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 830F PBT+PET (Europe-Africa-Middle East) PBT+PET, 30% Glass, Mold Release, Heat Stabilized, For food contact applications |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218 MT15 V 25 Black 21N PA66, 25/15% glass/mineral fiber, DRY Description: Polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 218 MT15.. |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Asia Pacific) Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | At 1 mm/min; ISO 527-2 |
Borealis Nepol™ GB402HP 40% Long Glass Fiber Reinforced Polypropylene Nepol GB402HP is a 40% long glass fiber reinforced polypropylene grade, produced using Borealis ` propriety and exclusive, patented Nepol technology intended for injection molding and extrusion. Th.. |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide RFC16 PA66/6, Glass/Carbon Fiber Filled, Injection Molded RFC16 is a Glass Fiber and Carbon Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as STAR C PA66 C 303VY Z3)Information provided by Eurostar. |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | ISO 527 |
Eurotec® Tecomid® NA40 GR25 NL XA60 PA6.6, 25% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural Information provided by Eurotec® |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | ISO 527-1/-2 |
DSM Akulon® S223-HM8 Nylon 66-40% Mineral Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TRV-4X9 PAMACM12-GF40 Product description: Grilamid TRV-4X9 is an amorphous, cycloaliphatic polyamide with 40% glass fibre reinforcement. Grilamid TRV-4X9 characterises itself through the following features: Very low shr.. |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | ISO 527 |
Eurotec® Tecotek® PC40 GR30 NL PC, 30% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | ISO 527-2 |
BASF Ultramid® T 4381 LDS 10/25% Glass/Mineral Filled PA6/6T (Dry) Description: Ultramid® T 4381 LDS is a semi-crystalline, partially aromatic high temperature polyamide (PA6/6T) for laser direct structuring (LPKFLDS®). As the material is reinforced with 10% fibe.. |
|||
Tensile Modulus | 9.00 GPa | 1310 ksi | ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 MW30 Polyamide 6 - Mineral Reinforced 30% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechani.. |