Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 8.67 GPa | 1260 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon PE002 PA 6 LNP* Stat-kon* PE002 is a compound based on Nylon 6 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americ.. |
|||
Tensile Modulus | 8.67 GPa | 1260 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon PE002 PA 6 (Asia Pacific) LNP* Stat-kon* PE002 is a compound based on Nylon 6 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Asia P.. |
|||
Tensile Modulus | 8.67 GPa | 1260 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp RFZ71S PA 66 LNP* Thermocomp* RFZ71S is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for t.. |
|||
Tensile Modulus | 8.67 GPa | 1260 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp RFZ71S PA 66 (Asia Pacific) LNP* Thermocomp* RFZ71S is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for t.. |