Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 8.65 GPa | 1250 ksi | STN EN ISO 527-2 |
Plastcom PLASTAMID® 6 GF 30 005 PA6 reinforced with glass fiber PA 6 for injection molding, reinforced with 30% glass fiber, used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools, hobby tools, gears, covers.. |
|||
Tensile Modulus | 8.65 GPa | 1250 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP KONDUIT MT00E PP LNP KONDUIT* MT00E is a compound based on Polypropylene resin containing 70% Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Tensile Modulus | 8.65 GPa | 1250 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP KONDUIT MT00E PP (Asia Pacific) LNP KONDUIT* MT00E is a compound based on Polypropylene resin containing Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Tensile Modulus | 8.65 GPa | 1250 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP KONDUIT MT00E PP (Europe-Africa-Middle East) LNP KONDUIT* MT00E is a compound based on Polypropylene resin containing Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |