Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 8.60 GPa | 1250 ksi | ASTM D638 |
Plenco Valite 1246-18X Novolac Phenolic, Granular, Injection Molded
(discontinued **) This Valite product has been replaced by Plenco 4246. Data provided by Plenco.VALITE 1246-18X is a black two-stage, medium heat resistant phenolic molding compound. It has excellent electrical, mol.. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | ASTM D638 |
Plenco Valite 4224 Novolac Phenolic, Granular, Transfer Molded
(discontinued **) This Valite product has been replaced by Plenco 4224. Data provided by Plenco.VALITE 4224 is a brown, two stage, general purpose phenolic molding compound. It has good electrical and moldability ch.. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® S3 GF 30 4 (3552) PA 6.10 Dry, 30% Glass Filled
(discontinued **) A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | 1 mm/min; ISO 527-1,-2 |
Lanxess Durethan® BKV 230 H2.0 DUS008 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibersInformation provided by LANXESS. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | d.a.m.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® DP BKV 30 XF 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, improved flowability, improved surface finishInformation provided by LANXESS. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | 1 mm/min; ISO 527-1,-2 |
Gromax BFG30-BN00N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | |
LATI Latilub 85-10T G/30 PES, 30% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyether Sulfone (PES). PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu.. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | |
LATI Latiohm 62-08 PD02 G/30 PPA, 30% Glass Fiber Reinforced Dissipative product based on Polyamide 6 (PA6). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | ISO R 527 |
Solvay TECHNYL® C 218 V 50 PA6, 50% glass fiber, Eh 50 Description: TECHNYL C 218 V50 is a polyamide 6 reinforced with 50% of glass fiber with excellent thermal stabilityColors: it is supplied in natural color and black color.Available in: Latin America.. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon DE002E PC (Europe-Africa-Middle East) LNP* STATKON* DE002E is a compound based on Polycarbonate resin containing Carbon Fiber. Added features include; Easy Molding.This data was supplied by SABIC-IP for the Europe-Africa-Middle East reg.. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DEL329EP PC (Europe-Africa-Middle East) LNP* STATKON* DEL329EP is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE, Flame Retardant. Added features include: Electrically Conductive, Internally Lubricated, Flame retard.. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON SE003 PA 12 (Europe-Africa-Middle East) LNP* Stat-kon* SE003 is a compound based on Nylon 12 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RF005SXS PA 66 LNP THERMOCOMP* RF005SXS is a compound based on Nylon 66 resin containing 25% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GFN3 PPE+HIPS (Asia Pacific) PPE+PS blend. 30% Glass reinforced.FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Suitable for fluid engineering applications including pump .. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RFB44XE PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RFB44XE is a compound based on Nylon 66 resin containing Glass Fiber, Glass Bead. Added features of this material include: Easy Molding. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | 1 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 226F5 Nylon 6.6, 25% Glass Fiber SAXAMID 226F5 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 25% glass fibers. It has high mechanical strength in combination with good flow properties.Information provid.. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | ASTM D638 |
Plenco 2000 Phenolic, Granular, Compression Molded PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under compo.. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | ASTM D638 |
Plenco 2308 Phenolic, Granular, Injection Molded PLENCO 02308 is a general purpose organic filled phenolic molding compound, offering improved heat resistance and optimized cure properties. UL recognized under component file E40654. 02308 is avai.. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | ISO 527 |
Polyram RamLloy A300NT Nylon 66/Polypropylene Alloy, 30% Glass Fiber Reinforced Nylon 66/PP alloy 30% glass fiber reinforced for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN FR52G20NH NC010 Polyphthalamide (PPA)
(Unverified Data**) 20% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G20NH NC010 is a 20% glass reinforced flame retardant lubricated high performance polyamide resin. It.. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R525 Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525 is hydrolysis-resistant, 25% glass-fiber reinforced PA66 resin. Available in natural it is lubricated for improved machine feed and flow. Glass-reinforced Vydyne resins provide higher .. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R525H BK02 Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H BK02 is high-flow, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R525H BK0201 Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H BK0201 is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R525H BLK Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H BLK is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R525H Nylon 66, 25% Glass Filled, Dry as Molded Vydyne® R525H is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties whe.. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® S3 GF 30 1 (3222) PA 6.10 Dry, 30% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66
(Unverified Data**) 25% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G25HSL NC010 is a 25% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform.. |
|||
Tensile Modulus | 8.60 GPa | 1250 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R525H Nat Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H Nat is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |