Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 8.50 GPa | 1230 ksi | 50 mm/min; ASTM D638 |
Ovation Polymers Opnyl OP66GF33 Nylon 66, 33% Glass Reinforced, Dry Nylon 66 - Glass reinforced (33 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. For Nylon compounds the .. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | ASTM D638 |
Premix Premi-Glas® 1206 LD Fiberglass Reinforced Thermoset SMC Premi-Glas® 1206 LD is a fiberglass reinforced thermoset sheet molding compound for transportation or structural and semi-structural applications where good surface appearance, high strength and du.. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527 |
Nilit FRIANYL A63 GV25 Nylon 6.6 for injection molding, 25% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527-2 |
PolyOne Nymax™ X GMF 604 40 UV Black 148 rev 4 Polyamide 6 (Nylon 6) The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor.. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527-1/-2 |
DSM Akulon® K224-HG8 (Cond.) 40% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527 |
Grupo Repol Dinalon® B1S25 G25 H PA6 25% Glass Fiber, Heat Stabilized Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | 1 mm/min; ISO 527-1,-2 |
Lanxess Durethan® AKV 30 G HR DUS023 900116 Nylon 66, 30% Glass Fiber PA 66, 30% glass fiber, injection molding, improved flowability, hydrolysis stabilized, improved surface finish, GIT/WITInformation provided by LANXESS. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527-1/-2 |
Lanxess Durethan® DP 1441/40 H2.0 EF 900116 Nylon 6, 40% Glass Fiber + Mineral PA 6, injection molding grade, 40% glass fibers/mineral, good heat-ageing resistance, good surface, good flowability (Easy Flow), low warpage |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527-1/-2 |
Lanxess Pocan® BF 4225 000000 PBT, 20% Glass Fiber PBT, 20% glass fibers, injection molding, flame retardant |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527 Type 1A |
Solvay TECHNYL® eXten D218 V30 Nylon 6.10, 30% glass fiber, DRY Description: TECHNYL® eXten D 218 V30 is a 30% Glass Fiber reinforced and heat stabilized product suitable to the manufacturing of all injection molded parts. This material is available in black... |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DE0029EF PC LNP STAT-KON* DE0029EF is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding. Flame Retardant, Electrically Conductive. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon EE002ER PEI (Europe-Africa-Middle East) LNP* Lubricomp* EFP36G is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding, Mold Release, Electrically Conductive.This data wa.. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP QF0069 PA6.10 (Europe-Africa-Middle East) LNP* THERMOCOMP* QF0069 is a compound based on PA610 resin contaning Glass Fiber, Flame Retardant. Added features include: Flame retardant. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP WF006L PBT LNP* THERMOCOMP* WF006L is a compound based on PBT resin containing 30% Glass Fiber. Added feature of this material is: Low Extractible. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | ASTM D638 |
Plenco 2308 Phenolic, Granular, Compression Molded PLENCO 02308 is a general purpose organic filled phenolic molding compound, offering improved heat resistance and optimized cure properties. UL recognized under component file E40654. 02308 is avai.. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | ASTM D638 |
Plenco 2408 Phenolic, Granular, Compression Molded PLENCO 02408 is a general purpose, organic filled phenolic molding compound, offering excellent cosmetic characteristics and improved electrical strength properties. UL recognized under component fi.. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | ASTM D638 |
Plenco 5488 Phenolic, Granular, Injection Molded PLENCO 05488 is a woodflour and graphite filled phenolic molding compound offering improved abrasion resistance. UL recognized under component file E40654. 05488 is available in brown. 05488 is not .. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | ASTM D638 |
Plenco 7021 Phenolic, Granular, Injection Molded PLENCO 07021 is a renumber of Plaslok 7021 which is the replacement material for the former Union Carbide BMRS-7021. It is a two-stage, impact grade phenolic molding compound suitable for compressio.. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527-1/-2 |
DSM Akulon® S223-HG7 (Cond.) 35% Glass Reinforced Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | cond; ISO 527-1/-2 |
DSM Novamid® 1010GN8-30 NAT PA6-GF30 FR 30% Glass Reinforced, Flame Retardant, Halogen free |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BG-25 S PA6-GF25 Product description: Grilon BG-25 S is a heat stabilized PA6 injection molding grade with 25 % glass fibers. Grilon BG-25 S has the following important properties: Excellent surface finishEasy flowi.. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® BG-40 HM PA6-GF40 Product description: Grilon BG-40 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 40% glass fibers. Grilon BG-40 HM has the following important prop.. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSGK-30 X PA666-(GF+GB)30 Product description: Grilon TSGK-30 X is a heat stabilized PA66 + PA6 injection molding grade with a 30% reinforcement combination (glass fibers and glass beads). Grilon TSGK-30 X has the following .. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® HR5330HF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)& 30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HF is a 30% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen.. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527 |
Eurotec® Tecodur® PB70 GR30 NL100 IL PBT, 30% glass fiber reinforced, impact modified, natural Information provided by Eurotec® |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® A3 GF 25 (2420) PA 6.6 Dry, 25% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527-1/-2 |
DSM Arnite® TV4 241 SL PBT-GF20 FR(17) 20% Glass Reinforced, Flame Retardant, UV Stabilized |