Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 8.33 GPa | 1210 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP DF005 PC LNP* Thermocomp* DF005 is a compound based on Polycarbonate containing 25% Glass Fiber. |
|||
Tensile Modulus | 8.33 GPa | 1210 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP DX10311 PC (Asia Pacific) DX10311 is 30% glass fiber reinforced, impact modified polycarbonate resin. High flow and good ductility. |
|||
Tensile Modulus | 8.33 GPa | 1210 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP PF005S PA 6 LNP* THERMOCOMP* PF005S is a compound based on Nylon 6 resin containing 25% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Tensile Modulus | 8.33 GPa | 1210 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP PF005S PA 6 (Asia Pacific) LNP* Thermocomp* PF005S is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |