Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 8.30 GPa | 1200 ksi | ISO 527, ASTM D638 |
Nilit Nilamid A G5 FR PH2 25% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous) Description: Nilamid A G5 FR PH2 combines flame retardancy with outstanding mechanical performance. This product has a complete yellow card, with RTI and CTI listings. The formulation has been optim.. |
|||
Tensile Modulus | 8.30 GPa | 1200 ksi | ISO 527 |
Nilit RECONYL B GV30 Recycled nylon 6 for injection molding, 30% glass fiber reinforced Recycled nylon 6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 8.30 GPa | 1200 ksi | |
Radici Radilon® A RV250 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Tensile Modulus | 8.30 GPa @Temperature 23.0 °C |
1200 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
PolyOne Bergamid™ B65 G30 black IG Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Tensile Modulus | 8.30 GPa @Temperature 23.0 °C |
1200 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
PolyOne Bergamid™ B700 G20 H UF Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Tensile Modulus | 8.30 GPa | 1200 ksi | ASTM D638 |
Shell Carilon® DP R1130 Polyketone, 30% Glass Fiber Reinforced
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON® Thermoplastic Polymer DP R1130 is a 30 percent glass fiber reinforced compound based on a developmental e.. |
|||
Tensile Modulus | 8.30 GPa | 1200 ksi | ASTM D638 |
Shell Carilon® DB6G6A10 Polyketone, 30% Glass-Reinforced General-Purpose Injection Molding Grade
(discontinue Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DB6G6A10 is a 30 percent short glass-fiber-reinforced, general purpose injection molding grade, wit.. |
|||
Tensile Modulus | 8.30 GPa | 1200 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® A-1115 HS Polyphthalamide (PPA) Resin, 15% Glass Reinforced, at 50% RH
(dis AMODEL A-1115 HS resin is a 15% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, and high tensile strength. Excellent cre.. |
|||
Tensile Modulus | 8.30 GPa | 1200 ksi | ASTM D638 |
Plenco Valite 424 Novolac Phenolic, Granular, Injection Molded
(discontinued **) This Valite product has been replaced by Plenco 2424. Data provided by Plenco.VALITE 424 is a black, two stage, general purpose phenolic molding compound. It has a good balance of properties for a .. |
|||
Tensile Modulus | 8.30 GPa | 1200 ksi | |
LATI Latishield 66-08A G/25-V0KB1 PA66, Steel/Glass Fiber Reinforced, Flame Retardant EMI shielding product based on Polyamide 66 (PA66). Steel fibers. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |
|||
Tensile Modulus | 8.30 GPa | 1200 ksi | ISO 527 Type 1A |
Solvay TECHNYL® C 216 V45 PA6, 45% glass fiber, Conditioned Description: Polyamide PA6, reinforced with 45% of glass fiber, for injection molding.Available in: EuropeProduct Applications: TECHNYL C 216 V45 has been optimized to have high impact strength, a n.. |
|||
Tensile Modulus | 8.30 GPa | 1200 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics SABIC STAMAX 40YM240 PP SABIC® STAMAX 40YM240 is a 40% long glass fiber reinforced polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMDS is 16497161... |
|||
Tensile Modulus | 8.30 GPa | 1200 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON RX06001 PA 66 (Europe-Africa-Middle East) LNP* Stat-kon* RX06001 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Easy Molding, High Impact, Electrically Conductive. |
|||
Tensile Modulus | 8.30 GPa | 1200 ksi | ASTM D638 |
Sumitomo Bakelite Durez® 118 Phenolic, Injection Grade Durez 118 Black Phenolic is a two-stage, asbestos free, general purpose molding material. It exhibits improved impact strength and resistance to flexural fatigue for demanding automotive, electrica.. |
|||
Tensile Modulus | 8.30 GPa | 1200 ksi | 1 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 226F4RY01 Nylon 6.6, 20% Glass Fiber SAXAMID 226F4RY01 is a polyamide 6.6 injection-molding-grade reinforced with 20% glass fibers. It has a halogen-free flame retardant.Information provided by SAX Polymers |
|||
Tensile Modulus | 8.30 GPa | 1200 ksi | ISO 527 Type 1A |
Solvay TECHNYL® C 246SI V30 PA6, 30% glass filled, DRY Description: Polyamide 6, reinforced with 30 % of glass fiber, with high impact resistance, for injection molding.Available in: Asia Pacific , Europe and North AmericaProduct Applications: Having go.. |
|||
Tensile Modulus | 8.30 GPa | 1200 ksi | ISO 527-1/-2 |
Suzhou Hipro Polymers Hiprolon® 70 MC HLS G30 Nylon 610, 30% glass fiber filled Hiprolon® 70 MC HLS G30 polyamide 6.10 compound reinforced with 30% chopped glass fiber for injection molding. Features: high heat resistance, dimension stability, impact resistance, good flow ab.. |
|||
Tensile Modulus | 8.30 GPa | 1200 ksi | ASTM D638 |
Plenco 2571 Phenolic, Granular, Compression Molded PLENCO 02571 is a general purpose, organic filled phenolic molding compound offering optimum cure characteristics while maintaining excellent mechanical and electrical properties. UL recognized unde.. |
|||
Tensile Modulus | 8.30 GPa | 1200 ksi | ASTM-D790 |
Polyram PlusTek PA4801G6 Nylon 6.6, 30% Glass Fiber Reinforced, PTFE lubricated 30% glass fiber reinforced, PTFE lubricated polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 8.30 GPa @Temperature 180 °C |
1200 ksi @Temperature 356 °F |
ISO 527-1/-2 |
DSM Stanyl® TW200B6 PA46-CF30 30% Carbon Reinforced, Heat Stabilized, Lubricated |
|||
Tensile Modulus | 8.30 GPa | 1200 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Minlon® 73GM40 NC010 Nylon 6
(Unverified Data**) 40% Mineral/Glass Reinforced Polyamide 6 Minlon 73GM40 NC010 is a 40% mineral/glass reinforced heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Poly.. |
|||
Tensile Modulus | 8.30 GPa | 1200 ksi | 1mm/min; ISO 527 |
BASF Ultramid® 8267G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid 8267G HS BK-102 is a heat stabilized, black pigmented, 40% mineral and glass fiber reinforced nylon 6 injection molding compound. It possesses a balance of engineering properties in combin.. |
|||
Tensile Modulus | 8.30 GPa | 1200 ksi | Elasticity; ISO 527-1/-2 |
BASF Ultrason S 2010 G6 30% Glass Filled PSU Ultrason S 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength. |
|||
Tensile Modulus | 8.30 GPa | 1200 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics SABIC STAMAX 40YM243 PP SABIC® STAMAX 40YM243 is a 40% long glass fiber reinforced UV stabilized polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMDS .. |