Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 8.24 GPa | 1200 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRILOY DF206XXH PC LNP* LUBRILOY* DF206XXH is a compound based on Polycarbonate containing 30% Glass Fiber, Proprietary Lubricant. Added features of this grade include: Wear Resistant, Healthcare. |
|||
Tensile Modulus | 8.24 GPa | 1200 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP MF006AL PP LNP* THERMOCOMP* MF006AL is a compound based on Polypropylene resin containing 30% Glass Fiber. Characteristics of this grade are: Low Extractable. |