Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.87 GPa | 1140 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD4413 PC Lexan* HFD4413 is a 30% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Tensile Modulus | 7.87 GPa | 1140 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD4413 PC (Asia Pacific) Lexan* HFD4413 is a 30% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Tensile Modulus | 7.87 GPa | 1140 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD4413 PC (Europe-Africa-Middle East) Lexan* HFD4413 is a 30% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |