Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.80 GPa | 1130 ksi | |
Plastcom SLOVAMID 66 GB 30 GF 20 PA66, 20% glass fibre, 30% glass beads FeaturesPA 66 chemically reinforced with 20% glass fibre and with the content of 30 % glass beads. Improved anisotropy of shrinkage. The relation of the anisotropy to the mechanical properties can b.. |
|||
Tensile Modulus | 7.80 GPa | 1130 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID 66 GF 25 Polyamide 66, 25% Glass Fiber FeaturesChemically reinforced with 25% glass fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Tensile Modulus | >= 7.80 GPa | >= 1130 ksi | ISO 527-1,2 |
Qualchem Danamid AFGFS2HUV30 Polyamide 66, 30% Glass Fiber Reinforced with glass fiber. Impact modified, heat and UV stabilized, for long-lasting use at 120-140°C, resistant to artificial lights.Information provided by Qualchem Zrt. |
|||
Tensile Modulus | 7.80 GPa @Thickness 4.00 mm, Temperature 23.0 °C |
1130 ksi @Thickness 0.157 in, Temperature 73.4 °F |
Injection Molded; ISO 527-2/1 |
PolyOne Bergamid™ B70 G30 grey VN7445CF Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Tensile Modulus | 7.80 GPa @Temperature 23.0 °C |
1130 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® LW9020FR BK851 PBT
(Unverified Data**) Crastin® LW9020FR BK851 is a 20% glass fiber reinforced, flame retardant, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional sta.. |
|||
Tensile Modulus | 7.80 GPa | 1130 ksi | cond.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® AKV 35 HR H2.0 901510 Nylon 66, Glass Fiber Reinforced PA 66, 35% glass fibers, injection molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS. |
|||
Tensile Modulus | 7.80 GPa | 1130 ksi | cond.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® BKV 40 H2.0 901510 Nylon 6, Glass Fiber Reinforced PA 6, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Tensile Modulus | 7.80 GPa | 1130 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 4521 PBT (Europe-Africa-Middle East) VALOX 4521 is a high flow, 19.5% glass reinforced flame retardant PBT injection moulding resin. Applications: electrical applications. |
|||
Tensile Modulus | 7.80 GPa | 1130 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON RX98063 PA 66 (Europe-Africa-Middle East) LNP* STAT-KON* RX98063 is a compound based on PA 66 resin containing Glass Fiber, Stainless Steel Fiber. Added features include; Antistatic. |
|||
Tensile Modulus | 7.80 GPa | 1130 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP DX99077 PC (Europe-Africa-Middle East) LNP* Thermocomp* DX99077 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Non-.. |
|||
Tensile Modulus | 7.80 GPa | 1130 ksi | ISO 527 Type 1A |
Solvay TECHNYL® AR 218 V25 Nylon 66, 25% glass fiber, DRY Description: Polyamide PA66 reinforced with 25% of glass fiber, heat stabilized, containing recycled material.Available in: Europe and North AmericaProduct Applications: TECHNYL® AR 218 V25 BLACK.. |
|||
Tensile Modulus | 7.80 GPa | 1130 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON RE002 PA 66 LNP* STAT-KON* RE002 is a compound based on Nylon 66 resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 7.80 GPa | 1130 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP IF006 PA6.12 (Europe-Africa-Middle East) LNP THERMOCOMP* IF006 is a compound based on nylon 6/12 resin containing glass fibre |
|||
Tensile Modulus | 7.80 GPa | 1130 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP NF0061 PC+ABS (Europe-Africa-Middle East) LNP* THERMOCOMP* NF0061 is a compound based on PC+ABS resin containing Glass Fiber, Flame Retardant. Added features include : Flame Retardant. |
|||
Tensile Modulus | 7.80 GPa | 1130 ksi | ASTM D638 |
Plenco 2535 Phenolic, Granular, Injection Molded PLENCO 02535 is a general purpose, organic filled phenolic molding compound offering optimized cure characteristics and excellent electrical properties. Type ASTM 5948 CFG, and UL recognized under c.. |
|||
Tensile Modulus | 7.80 GPa | 1130 ksi | ASTM D638 |
Plenco 7200 Phenolic, Granular, Injection Molded PLENCO 07200 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength, good powder properties and excellent cosmetic properties. UL recognized under component .. |
|||
Tensile Modulus | 7.80 GPa | 1130 ksi | DIN EN ISO 527 |
Wolf Kunststoff ZEDEX® ZX-324VMT A3B PEEK, Fiber Reinforced Main Characteristics: Maximum rigidity; Very good wear resistance; Low stick-slip tendency; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInfor.. |
|||
Tensile Modulus | 7.80 GPa | 1130 ksi | ASTM D638 |
Plenco 2300 Phenolic, Granular, Transfer Molded PLENCO 02300 is a general purpose organic filled molding compound formulated to offer excellent processability while maintaining mechanical strength values. UL recognized under component file E40654.. |
|||
Tensile Modulus | 7.80 GPa | 1130 ksi | ISO 527-1/-2 |
DSM Stanyl® TW200FM33 Nylon 46-30% Glass and Mineral Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Tensile Modulus | 7.80 GPa | 1130 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® LV-3 ESD PA12-GF30 Product description: Grilamid LV-3 ESD is an antistatic PA12 injection molding grade, with fiber reinforcement of 30%. Due to its special formulation, the material can be used for applications where.. |
|||
Tensile Modulus | 7.80 GPa | 1130 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® LW9020FR BK851 PBT+ASA
(Unverified Data**) 20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020FR BK851 is a 20% glass fiber reinforced flame retardant black polybutylene tere.. |
|||
Tensile Modulus | 7.80 GPa | 1130 ksi | ASTM D638 |
Azdel SuperLite® SL552000-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness) AZDEL SuperLite® SL552000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Tensile Modulus | 7.80 GPa | 1130 ksi | ISO 527-1 |
Barlog Plastics KEBATER BFA20 PBT, 20% glass fiber reinforced, flame retardant PBT-GF20 FRInformation provided by BARLOG plastics GmbH. |
|||
Tensile Modulus | 7.80 GPa | 1130 ksi | 1 mm/min |
Arkema Group Rilsan® BZM 30 TL Nylon 11, 30% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA11,MHL,18-050,GF30Rigid grade with glass fiber (30%) filler for injection molding. Available colors: black and natural. Light and heat stabilized.Rigidity. High compressive st.. |
|||
Tensile Modulus | 7.80 GPa | 1130 ksi | 1mm/min; ISO 527 |
Teijin Panlite® BS-8110R Friction and Abrasion Resistant, Carbon Fiber Reinforced Polycarbonate Resin CF 10% reinforced grade, meeting UL 94 V-2. it is compounded with fluorine powder to improve friction and abrasion resistance and also exhibits a mold release property, maintaining excellent charact.. |
|||
Tensile Modulus | 7.80 GPa | 1130 ksi | ISO 527-1/-2 |
Suzhou Hipro Polymers Hiprolon® 90 MC HLS G30 Nylon 612, 30% glass fiber filled Hiprolon® 90 MC HLS G30 is a polyamide 6.12 compound reinforced with 30% chopped glass fiber, and is used for injection molding. Features: high dimension stability, chemical resistance, impact resi.. |