Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.79 GPa | 1130 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Stat-Tech™ PC-15CF/000 Black Polycarbonate (PC) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Tensile Modulus | 7.79 GPa | 1130 ksi | ASTM D638 |
Qualchem Danaprop PP1GF-30 Polypropylene, 30% Glass Fiber Polypropylene (co-polymer) reinforced with glass fiberInformation provided by Qualchem Zrt. |
|||
Tensile Modulus | 7.79 GPa | 1130 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AS-40GF/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 7.79 GPa | 1130 ksi | ASTM D1708 |
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus with .. |
|||
Tensile Modulus | 7.79 GPa | 1130 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY DF2049 PC LNP* LUBRILOY* DF2049 is a compound based on Polycarbonate resin containing 20% Glass Fiber, Proprietary Lubricant. Added features include: Wear Resistant, Flame Retardant. |
|||
Tensile Modulus | 7.79 GPa | 1130 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY DF2049 PC (Asia Pacific) LNP* Lubriloy* DF2049 is a compound based on Polycarbonate resin containing Glass Fiber, Proprietary Lubricant. Added features of this material include: Internally Lubricated, Flame Retardant. |
|||
Tensile Modulus | 7.79 GPa | 1130 ksi | ASTM D638 |
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI) Torlon® 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus w.. |
|||
Tensile Modulus | 7.79 GPa | 1130 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp OK006 PPS - Linear LNP* Thermocomp* OK006 is based on a Linear Polyphenylene Sulfide (PPS) containing Talc.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 7.79 GPa | 1130 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing 20% Long Glass Fiber. Added features of this material include: Easy Molding, Structural. |
|||
Tensile Modulus | 7.79 GPa | 1130 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS (Europe-Africa-Middle East) LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Tensile Modulus | 7.79 GPa | 1130 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DEP32 PC LNP* STAT-KON* DEP32 is a compound based on Polycarbonate containing 10% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Tensile Modulus | 7.79 GPa | 1130 ksi | Storage |
Epoxy Technology EPO-TEK® TV1002 Polyimide Adhesive Material Description: A single component, screen printable polyimide adhesive designed for semiconductor wafer passivation applications. It is a high temperature chemistry capable of resisting >400.. |
|||
Tensile Modulus | 7.79 GPa | 1130 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS (Asia Pacific) LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing Long Glass. Added features of this material include: Easy Molding. |