Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.60 GPa | 1100 ksi | STN EN ISO 527-2 |
Plastcom SLOVALEN PH 69 GF 40 Polypropylene Homopolymer, 40% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 40% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Tensile Modulus | 7.60 GPa | 1100 ksi | |
Plastcom SLOVAMID 6 NG1 GF 20 HLS PA6, 20% glass fibre, combined stability FeaturesPA 6 for injection moulding, chemically strengthened with 20% glass fibre, heat and wheather stabilized. Stabilized against hydrolisys. Good surface finisch. Scratch resistent.Packaging, tra.. |
|||
Tensile Modulus | 7.60 - 11.7 GPa | 1100 - 1700 ksi | ASTM D638 |
Proto3000 Accura® Bluestone™ Stereolithography (SLA) Prototyping Polymer Description: A high stiffness engineered nanocomposite that opens new applications for stereolithography users. Features:Exceptional stiffnessHigh temperature resistanceExcellent accuracyHigh humidi.. |
|||
Tensile Modulus | 7.60 GPa | 1100 ksi | |
Radici Radilon® A RV300 990 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Tensile Modulus | 7.60 GPa | 1100 ksi | ISO 527-1/-2 |
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Milled Glass Fiber PA 6, injection molding grade, 30% milled fibers, UL 94V-2 at 0.8 mm, max. temperature in glow wire test: 960 °C at 0,75 mm, "halogen-free", good heat-ageing resistanceApplication Examples: Medic.. |
|||
Tensile Modulus | 7.60 GPa | 1100 ksi | 1 mm/min; ISO 527-1,-2 |
Lanxess Durethan® DP 2131/20 H3.0 000000 Nylon 6, 20% Glass Fiber PA 6, 20% glass fiber, injection molding, heat-ageing stabilized, weather stabilized, improved surface finishInformation provided by LANXESS. |
|||
Tensile Modulus | 7.60 GPa | 1100 ksi | ISO 527-1/-2 |
Lanxess Durethan® DP 2131/20 W1 901317 Nylon 6, 20% Glass Fiber PA 6, injection molding grade, 20% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 20 H2.0, weather resistance, good heat-ageing resistance |
|||
Tensile Modulus | 7.60 GPa | 1100 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218G V33 Black 34N PA66, 25% glass fiber, Conditioned Description: Polyamide 66, reinforced with 25% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. Avail.. |
|||
Tensile Modulus | 7.60 GPa | 1100 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP MFL36S PP LNP* LUBRICOMP* MFL36S is a compound based on Polypropylene resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
Tensile Modulus | 7.60 GPa | 1100 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP HF008 PA 11 (Asia Pacific) LNP* THERMOCOMP* HF008 is a compound based on Nylon 11 resin containing Glass Fiber. |
|||
Tensile Modulus | 7.60 GPa | 1100 ksi | ASTM D638 |
Sumitomo Bakelite Durez® 22257 Phenolic, Compression Grade Durez 22257 Black Phenolic is a two-stage, asbestos-free, medium impact molding material. It is designed for appliance and electrical applications where additional mechanical strength is required. .. |
|||
Tensile Modulus | 7.60 GPa | 1100 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP ZX09022 PPE+PP (Europe-Africa-Middle East) Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod.. |
|||
Tensile Modulus | 7.60 GPa | 1100 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOTUF WF006I PBT (Europe-Africa-Middle East) LNP* Thermotuf* WF006I is a compound based on Polybutylene Terephalate resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Tensile Modulus | 7.60 GPa | 1100 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP HF008 PA11 LNP THERMOCOMP* HF008 is a compound based on Nylon 11 resin containing 40% Glass Fiber. |
|||
Tensile Modulus | 7.60 GPa | 1100 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP MF006SXP PP LNP THERMOCOMP* MF006SXP is a compound based on Polypropylene resin containing 30% Glass Fiber. Added features of this material include: Chemically Coupled. |
|||
Tensile Modulus | 7.60 GPa | 1100 ksi | ASTM D638 |
Sumitomo Bakelite Durez® 22257 Phenolic, Injection Grade Durez 22257 Black Phenolic is a two-stage, asbestos-free, medium impact molding material. It is designed for appliance and electrical applications where additional mechanical strength is required. .. |
|||
Tensile Modulus | 7.60 GPa | 1100 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus .. |
|||
Tensile Modulus | 7.60 GPa | 1100 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP (Asia Pacific) Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus .. |
|||
Tensile Modulus | 7.60 GPa | 1100 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP (Europe-Africa-Middle East) Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus .. |
|||
Tensile Modulus | 7.60 GPa | 1100 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PPX ZX09022 PPE+PP (Europe-Africa-Middle East) Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod.. |
|||
Tensile Modulus | 7.60 GPa | 1100 ksi | ASTM D638 |
Plenco 7202 Phenolic, Granular, Injection Molded PLENCO 07202 is an organic fiber reinforced phenolic molding compound, formulated to offer improved mechanical strength properties with an industrial finish. UL recognized under component file E4065.. |
|||
Tensile Modulus | 7.60 GPa | 1100 ksi | ISO 527 |
Polyram PlusTek PD502G6 Nylon 12 for Injection Molding, 30% Glass-fiber Reinforced 30% Glass-fiber reinforced, V-0 1.6 mm, Nylon 12 for injection molding application.Information provided by Polyram. |
|||
Tensile Modulus | 7.60 GPa | 1100 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 GVS 10/30 HWCP 10% Glass Fiber and 30% Glass Sphere Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 7.60 - 11.7 GPa | 1100 - 1700 ksi | ASTM D638 |
3D Systems Accura® Bluestone™ Plastic for SLA® Systems A high stiffness engineered nanocomposite that opens new applications for stereolithography users. For use with solid-state stereolithography (SLA®) systems.ApplicationsWind-tunnel testing for the .. |
|||
Tensile Modulus | 7.60 GPa | 1100 ksi | |
BASF Procom® GC40S 402 Polypropylene Uses: Electrical appliance housings (e.g. drills), components requiring high impact and temperature resistance, furniture frames.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 7.60 GPa | 1100 ksi | ASTM D638 |
PolyOne Stat-Tech™ MP-25NCF/000 Modified PPO - 25% Nickel Coated Graphite Fiber
(discontinued **) Data provided by PolyOne. |
|||
Tensile Modulus | 7.60 GPa | 1100 ksi | ASTM D638 |
PolyOne Edgetek® MP-30GF/000 Modified PPO - 30% Glass Fiber Reinforced
(discontinued **) Data provided by PolyOne. |