Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.43 GPa | 1080 ksi | 1 mm/min |
Arkema Group Rilsan® AZM 30 NOIR T6LD Nylon 12, 30% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-060,GF30Rigid grade with glass fiber (30%) for injection molding. Available color: black. Reinforced light and heat stabilizing agent. Mold-release agent.High rigid.. |