Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.30 GPa @Temperature 23.0 °C |
1060 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® LW9320 BK851 PBT
(Unverified Data**) Crastin® LW9320 BK851 is a 20% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp.. |
|||
Tensile Modulus | 7.30 GPa @Temperature 23.0 °C |
1060 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® LW9320LM BK591 PBT
(Unverified Data**) Crastin® LW9320LM is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. It has excellent surface aspect, dimensional stability and low warpage and was developed fo.. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | ISO 527 |
Nilit FRIANYL C73 HS-GV30 Nylon 6.6/6 for injection molding, 30% glass fiber reinforced Nylon 6.6/6 for injection molding, medium viscosity, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | ASTM D638 |
Solvay Specialty Polymers Radel® R-7120 Polyphenylsulfone, 20% glass fiber
(discontinued **) RADEL R 7120 is a 20% glass fiber reinforced grade of RADEL R polyphenylsulfone developed specifically for aircraft interior applications. The product complies with the FAA regulation 14CFR Part 25 .. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | |
Idemitsu Kosan Xarec® N WA 7020 SPS, 20% Glass Filled Crystalline Polymer Blend, Glass Filled, Impact Modified. Used in Automotive Electronics applications. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | ISO 527 |
Idemitsu Kosan Xarec® WA 204 SPS, 20% Glass Filled Crystalline Polymer, Glass Filled, Impact Modified. Used in Automotive and Industrial applications. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | |
Idemitsu Kosan Xarec® WA 210 SPS, 20% Glass Filled Crystalline Polymer, Glass Filled, Impact Modified, Improved Mold Release. Used in Automotive and Industrial applications. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | cond.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® BKV 25 F30 000000 Nylon 6, Glass Fiber Reinforced, Flame Retardant PA 6, 25% glass fibers, injection molding, flame retardantInformation provided by LANXESS. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | 1 mm/min; ISO 527-1,-2 |
Gromax BFG30-DN00N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | ISO 527 Type 1A |
Solvay TECHNYL® C 216 V40 PA6, 40% glass fiber, Conditioned Description: TECHNYL® C 216 V40 is a polyamide 6, reinforced with 40% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers a good combinati.. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RF004 PA 66 LNP THERMOCOMP* RF004 is a compound based on Nylon 66 resin containing 20% Glass Fiber. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RF004XXD PA 66 LNP THERMOCOMP* RF004XXD is a compound based on Nylon 66 resin containing 20% Glass Fiber. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | 1 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 226F4 Nylon 6.6, 20% Glass Fiber SAXAMID 226F4 is a polyamide 6.6 injection-molding-grade reinforced with 20% glass fibers.Information provided by SAX Polymers |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl GFN1430V PPE+PS Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable.. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GTX GTX830 PPE+PA (Europe-Africa-Middle East) NORYL GTX830 a 30% glass reinforced grade which offers an excellent combination of chemical/heat resistance in combination with stiffness. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP MF006SXP PP LNP THERMOCOMP* MF006SXP is a compound based on Polypropylene resin containing 30% Glass Fiber. Added features of this material include: Chemically Coupled. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl GFN1430V PPE+PS (Asia Pacific) Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable.. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | ASTM D638 |
Plenco 2369 Phenolic, Granular, Transfer Molded PLENCO 02369 is a general purpose, organic filled phenolic molding compound, formulated to minimize the generation of free ammonia for applications that are sensitive to such formation. PLENCO 02369.. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | ISO 527-1/-2 |
Unitika BV2120G15 PA66, 15% Glass Fiber Reinforced, Flame Retardant, Dry Information provided by Unitika Ltd. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | ASTM-D790 |
Polyram Polytron P40B03 Copolymer Polypropylene, Chemically Coupled 40% Long Glass Fiber A CHEMICALLY COUPLED 40% LONG GLASS FIBERS REINFORCED BLACK POLYPROPYLENE, HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.These products have significantly improved impact performance characteris.. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | ISO 527-1/-2 |
DSM Akulon® K224-HG4 Nylon 6-20% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® LW9320LM BK591 PBT+SAN
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9320LM is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. It ha.. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | 1 mm/min |
Arkema Group Rilsan® BZM 23 G9 Nylon 11, 23% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA11,MS,18-040,(G+C)(F+D)(25+05)Rigid grade with glass fiber (23%) and graphite filler for injection molding. Available color: steel black gray. Additive free.Rigidity. Low fric.. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | ISO 527-1 |
Barlog Plastics KEBAFORM C 2527 POM Copolymer, 25% glass fiber reinforced POM-GF25Information provided by BARLOG plastics GmbH. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | ISO 527-1/-2 |
BASF Ultrason® E 2010 G4 MR SW 15102 20% Glass Filled PESU Information provided by BASF |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® B3 GF 35 (2473) PA 6 Conditioned, 35% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Tensile Modulus | 7.30 GPa | 1060 ksi | ASTM D638 |
Plenco 7321 Phenolic, Nodular, Injection Molded PLENCO 07321 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength and excellent dimensional stability. Type ASTM 5948 CFI-5, and UL recognized under compon.. |