Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.20 GPa | 1040 ksi | STN EN ISO 527-2 |
Plastcom SLOVASTER® B GF 20 Polybutylene Terephthalate, 20% Glass Fiber FeaturesPBT for injection moulding, chemically reinforced with 20% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a.. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | |
Plastcom SLOVASTER® B1 HML GF 20 PBT, 20% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | |
Radici Radilon® S RV200 (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | ISO 527-2/1A |
Radici Raditer® B RV 200 Polybutylene Terephthalate with 20% Glass fiber Raditer® B RV 200 is a glass fiber reinforced thermoplastic polyester based on polybutylene terephthalate. The PBT compounds combine excellent thermal, mechanical, electrical and chemical properti.. |
|||
Tensile Modulus | 7.20 GPa @Thickness 4.00 mm, Temperature 23.0 °C |
1040 ksi @Thickness 0.157 in, Temperature 73.4 °F |
ISO 527-2/1 |
PolyOne Bergadur™ PB40 G15 U SO1 BK Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | STN EN ISO 527-2 |
Plastcom SLOVALEN PH 49 GF 30 003/3M Polypropylene reinforced with glass fiber, heat stabilized Modified homopolymer PP for injection molding, reinforced with 30% glass fiber, heat stabilized. Delivered in black color.Information Provided by Plastcom spol. s r.o. |
|||
Tensile Modulus | 7.20 GPa @Temperature 23.0 °C |
1040 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® SK642FR BK851 PBT
(Unverified Data**) Crastin® SK642FR BK851 is a black 15% glass fiber reinforced, flame retardant polybutylene terephthalate for injection molding. It has a UL94 V-0 rating @ 0.75mm.Information provided by DuPont Perf.. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | ISO 527-1/-2 |
DSM Akulon® S223-HPG8U (Cond.) 43% Glass Reinforced, Impact Modified Nylon 66 (North America)
(discontinued * Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM CRS5201R PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. Resin is RoHS com.. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 412 PBT (Europe-Africa-Middle East) VALOX 412 is 20% glass reinforced PBT injection moulding resin. Applications: Spotlights, appliance housings and handles. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 412 PBT (Europe-Africa-Middle East) VALOX 412 is 20% glass reinforced PBT injection moulding resin. Applications: Spotlights, appliance housings and handles. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP KF004 Acetal Copolymer (Europe-Africa-Middle East) LNP* THERMOCOMP* KF004 is a compound based on Acetal Copolymer containing Glass Fiber. Added features include : Chemically Coupled. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | ISO 527-1/-2 |
DSM Akulon® F249-HG4 Nylon 6-20% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-2H black PA*-GF20 Product description: Grivory GV-2H is a 20% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide. Grivory.. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-2H PA*-GF20 Product description: Grivory GV-2H natural is a 20% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide... |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® SK642FR NC010 Polybutylene Terephthalate (PBT) 15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK642FR is a 15% glass fibre reinforced flame retardant polybutylene terephthalate for injection moulding.It has a UL94 V-0 ra.. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 70G30HSLR BK099 Nylon 66
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G30HSLR BK099 is a 30% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection mol.. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 70G30L NC010 Nylon 66
(Unverified Data**) 30% Glass Reinforced Polyamide 66Zytel 70G30L NC010 is a 30% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide RFB53U PA66, 50% Glass Bead/Fiber Filled, Injection Molded RFB53U is a Glass Bead/ Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 1525 VK Z4)Information provided by Eurostar. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | ISO 527-1/-2 |
BASF Ultramid® B3EG7 BK 00564 35% Glass Filled PA6 (Conditioned) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | 1 mm/min |
Arkema Group Orgalloy® R 6030 Nylon 6 Alloy, 30% Glass fiber (Conditioned) Rigid polyamide 6 alloy: easy to process, low moisture absorption, chemical resistance (no known solvents).Special 30% glass fiber reinforced for overmolding with modified PP.ISO data provided by th.. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® A3 GF 20 (2419) PA 6.6 Dry, 20% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® VX4920 PBT (Europe-Africa-Middle East) VALOX VX4920 is a 20% glass reinforced nucleated PBT/ASA blend with excellent mechanical properties, high dimensional stability and low density. Applications: connectors and automotive industry. |
|||
Tensile Modulus | 7.20 GPa | 1040 ksi | ISO 527-2 |
Pasargad Polymer Peyvand Pasamid 3P-L1130B Nylon 6, 30% Glass Fiber Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co |