Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.77 GPa | 981 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® GP-5300G PBT, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 6.77 GPa | 981 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® GP-5300G PBT, Glass Filled Information provided by Samsung Cheil Industries. |