Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.25 GPa | 906 ksi | 50 mm/min; ASTM D638 |
Ovation Polymers Nemcon™ H PK DP110/X5 PEEK Thermally Conductive Polyetheretherketone, excellent chemical, high stiffness, modulus and HDT.Information provided by Ovation Polymers |
|||
Tensile Modulus | 6.25 GPa | 906 ksi | 50 mm/min; ASTM D638 |
Ovation Polymers Nemcon™ H PK DP110/X5 Polyetheretherketone Thermally Conductive Polyetheretherketone, excellent chemical, high stiffness, modulus and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All sa.. |
|||
Tensile Modulus | 6.25 GPa | 906 ksi | |
Radici Radilon® S CP400 (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Tensile Modulus | 6.25 GPa | 906 ksi | |
Radici Radilon® S RCP3010LK (cond.) Nylon 6 PA6 30% Glass Fiber and mineral filler reinforced injection molding grade. Good stiffness and good dimensional stability. Heat stabilized, good surface finish.Information provided by Radici group. |
|||
Tensile Modulus | 6.25 GPa | 906 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP PH0240A PA 6 LNP* THERMOCOMP* PH0240A is a compound based on Nylon 6 resin. Added features of this grade include: High Impact, High Specific Gravity. |
|||
Tensile Modulus | 6.25 GPa | 906 ksi | Storage |
Epoxy Technology EPO-TEK® H31D Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H31D is a single component, electrically conductive silver epoxy designed for die-bonding of semiconductors, including IC’s, resistors, capacitors, transistors, and d.. |
|||
Tensile Modulus | 6.25 GPa | 906 ksi | ISO 527 |
Eurotec® Tecolen® HP10 GR30 NL HS PPCP, 30% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Tensile Modulus | 6.25 GPa | 906 ksi | ISO 527 |
Eurotec® Tecomid® NA40 GR15 NL HS PA6.6, 15% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Tensile Modulus | 6.25 GPa | 906 ksi | ISO 527 |
Eurotec® Tecomid® NA40 GR15 NL PA 6.6 15% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Tensile Modulus | 6.25 GPa | 906 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Valox® V9235 PET (Europe-Africa-Middle East) Valox heat stabilized, 15% Glass filled grade with mold release based on recycle PET. This grade is typically applied for business Machines applicationsThis data was supplied by SABIC-IP for the Eu.. |