Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.21 GPa | 901 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ 80520 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 6.21 GPa | 900 ksi | ASTM D638 |
Polymer Resources ABS-G20 ABS, 20% Glass Reinforced Acrylonitrile Butadiene Styrene, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Tensile Modulus | 6.21 GPa | 900 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AS-13CF/000 Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 6.21 GPa | 900 ksi | ASTM D638 |
Fiberfil® J-60/30/E/M Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 6.21 GPa @Temperature 175 °C |
901 ksi @Temperature 347 °F |
4; ISO 527-2 |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica.. |
|||
Tensile Modulus | 6.21 GPa | 900 ksi | ASTM D638 |
Plastics Group Polifil® GFABS-20 20% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS) Polifil® GFABS series compounds combine the most desirable properties of both components - allowing for enhanced processability and toughness together with the stiffness of glass.Applications: Fire.. |
|||
Tensile Modulus | 6.21 GPa | 900 ksi | ASTM D638 |
Ensinger Tecatron® XP-64 Compression Molded PPS Compound, 40% Fiberglass Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Tensile Modulus | 6.21 GPa | 900 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AT-25GF/000 Acetal-Copolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 6.21 GPa | 900 ksi | TM R050-36 |
Resinlab® EP1285HD-14 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |