Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.70 GPa | 827 ksi | |
Plastcom SLOVALEN PH 49 GF 25 PP, 25% glass fibre, mod. of mech. properties FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 25 % glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID 6 GF 15 LS Polyamide 6, 15% Glass Fiber, UV Stabilization FeaturesPA 6 for injection moulding, chemically reinforced with 15% glass fiber, stabilized against UV-radiation. Used for the grips of electric tools, hobby tools, gears, covers of electric tools... |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | 50 mm/min; ASTM D638 |
Ovation Polymers Opnyl OP6GF43 Nylon 6, 43% Glass Reinforced, Conditioned Nylon 6 - Glass reinforced (43 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. For Nylon compounds the m.. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | ISO 527-1,2 |
Qualchem Danamid FGF-10 Polyamide 6, 10% Glass Fiber Reinforced with glass fiber.Information provided by Qualchem Zrt. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | ISO 527-1,2 |
Qualchem Danamid FGF-15 Polyamide 6, 15% Glass Fiber Reinforced with glass fiber.Information provided by Qualchem Zrt. |
|||
Tensile Modulus | 5.70 GPa @Temperature 23.0 °C |
827 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
PolyOne Bergamid™ B65 G/Mi20 UF grey LS Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Tensile Modulus | 5.70 GPa @Temperature 23.0 °C |
827 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® SK602 BK851 PBT
(Unverified Data**) Crastin® SK602 BK851 is a 15% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP BG004 SAN (Europe-Africa-Middle East) LNP* LUBRICOMP* BG004 is a compound based on Styrene Acrylonitril resin containing Graphite. Added features include: Internally Lubricated. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® BKV 30 EF 000000 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers, low viscosity (Easy Flow) |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® DP BKV 240 H2.0 901510 Copolyamide, 40% Glass Fiber CoPA, injection molding grade, 40% glass fibers reinforced, elastomer-modified, good heat-ageing resistance |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | ISO 527-1/-2 |
Lanxess Pocan® B 4215 000000 PBT, 12% Glass Fiber PBT, 12% glass fibers, injection molding, flame retardant |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | ISO 527-1/-2 |
Lanxess Pocan® BF 4215 000000 PBT, 12% Glass Fiber PBT, 12% glass fibers, injection molding, flame retardant |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | ISO 527-1/-2 |
Lanxess Durethan® BKV 115 000000 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 15, even in.. |
|||
Tensile Modulus | 5.70 GPa @Temperature 80.0 °C |
827 ksi @Temperature 176 °F |
1 mm/min; ISO 527 |
SABIC Innovative Plastics SABIC STAMAX 40YM240 PP SABIC® STAMAX 40YM240 is a 40% long glass fiber reinforced polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMDS is 16497161... |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP LF002 PEEK (Europe-Africa-Middle East) LNP* THERMOCOMP* LF002 is a compound based on Polyetheretherketone resin contaninig Glass Fiber. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP MF006SXP PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MF006SXP is a compound based on Polypropylene resin containing Glass Fiber. Added features include: Chemically Coupled. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp MX06050 PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MX06050 is a compound based on Polypropylene resin containing Glass Fiber. Added features include; Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp PFB42ES PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PFB42ES is a compound based on PA6 resin containing Glass Fiber, Glass Bead. Added features include: Easy Molding, Heat Stabilized.This data was supplied by SABIC-IP for the Europe-.. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp ZF004XXC PPE+PS (Europe-Africa-Middle East) LNP* THERMOCOMP* ZF004XXC is a compound based on PPE+PS Blend resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | dry; ISO 527-1/-2 |
DSM Akulon® K222-KGV4 /A PA6-GF20 FR(30) 20% Glass Reinforced, Heat Stabilized, Flame Retardant (Halogen-phosphorous-free) |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | cond; ISO 527-1/-2 |
DSM Novamid® 1010GH30 NAT PA6-GF30 30% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | cond; ISO 527-1/-2 |
DSM Novamid® 1013GH30 1 NA/BK701 PA6-GF30 30% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Tensile Modulus | 5.70 GPa @Temperature 180 °C |
827 ksi @Temperature 356 °F |
ISO 527-1/-2 |
DSM Stanyl® TE200F8 PA46-GF40 40% Glass Reinforced, Heat Stabilized, for E&E applications |
|||
Tensile Modulus | 5.70 GPa @Temperature 160 °C |
827 ksi @Temperature 320 °F |
ISO 527-1/-2 |
DSM Stanyl® TW271B3 (PA46+PTFE)-CF15 15% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® LV-3A H PA12-GF30 Grilamid LV-3A H is a 30 % glass fibre reinforced PA12 for injection moulding. Grilamid LV-3A H is very stiff and tough and offers an improved hydrolysis resistance compared to standard PA12 GF 30.I.. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TSGK-30 X PA666-(GF+GB)30 Product description: Grilon TSGK-30 X is a heat stabilized PA66 + PA6 injection molding grade with a 30% reinforcement combination (glass fibers and glass beads). Grilon TSGK-30 X has the following .. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | 1 mm/min; ISO 527 |
Eurostar Starpylen MX06050 PP, 30% Glass Filled, Injection Molded Starpylen MX06050 is a 30% Glass Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | |
BASF Procom® GC30S 401 Polypropylene Uses: Electrical appliance housings (e.g. drills), components requiring high impact and temperature resistance, furniture frames.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | dry; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 GF15 Polyamide 6 - Glass Fiber Reinforced 15% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6
(Unverified Data**) 30% Glass Reinforced Toughened Polyamide 6 Zytel 73G30T NC010 is a 30% glass fiber reinforced toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |