Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.60 GPa | 812 ksi | STN EN ISO 527-2 |
Plastcom SLOVASTER® B GF 15 Polybutylene Terephthalate, 15% Glass Fiber FeaturesPBT for injection moulding, chemically reinforced with 15% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a.. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | 50 mm/min; ASTM D638 |
Ovation Polymers Nemcon™ E PC 08CF Polycarbonate Nemcon E-series products are designed for use in ESDA electronic assembly environments where strict control of ESD and cleanliness are critical. Nemcon E PC 08CF is a carbon fiber-reinforced polyca.. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP AFP26 ABS (Europe-Africa-Middle East) LNP* Lubricomp* AFP26 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, PTFE, Silicone. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | ISO 527-1/-2 |
Lanxess Durethan® BKV 115 H2.0 901510 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 15, even in.. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® BKV 330 H2.0 901510 Nylon 6, 30% Glass Fiber PA 6, injection molding type, 30% glass fibers, branched/structural viscosity, good weldability (vibration or hot plate), good heat-ageing resistance |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | |
LATI Latilub 73/13-15T G/15 POM, 15% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyoxymethylene (POM). PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus.. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP KF002L Acetal Homopoly LNP* THERMOCOMP* KF002L is a compound based on Acetal Homopolymer resin containing 10% Glass Fiber. Added features of this material include: Low Extractible. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP MFB44S PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MFB44S is a compound based on Polypropylene resin containing Glass Fiber, Glass Beads. Added features include; Heat Stabilized, Cu-Stabilized. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX.. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | ISO 527-1/-2 |
Unitika A1022GFL15 PA6, 15% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | ASTM-D790 |
Polyram PlusTek PB302G3 Nylon 6, 15% Glass Fiber 15% glass-fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | 1mm/min; ISO 527-2 |
Borealis Xmod™ GD302HP Polypropylene, Glass Fiber Reinforced Xmod™ GD302HP is a 30 % chemically coupled high performance glass fiber reinforced polypropylene compound intended for injection molding. This material has an excellent balance between impact stre.. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | ISO 527 |
Polyram Polytron P30N03 Polypropylene, 30% Long Glass Fibers A chemically coupled 30% long glass fibers reinforced natural polypropylene, heat stabilized, for injection molding applications. These products have significantly improved impact performance chara.. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | ISO 527-1/-2 |
DSM Akulon® S223-G4U (Cond.) 23% Glass Reinforced Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 5.60 GPa @Temperature 180 °C |
812 ksi @Temperature 356 °F |
ISO 527-1/-2 |
DSM Stanyl® OCD2300 BLK PA46-GF50 50% Glass Reinforced, Heat Stabilized |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 GV 25 HWCP 25% Glass Fiber Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® EBV-15H black 9697 PA6-GF15 Product description: Grilon EBV-15H black 9697 is a high viscosity, heat stabilized PA6 extrusion blow molding grade with 15% glass fibers. Grilon EBV-15H black 9697 has the following important prop.. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TSG-25/4 PA666-GF25 Information provided by EMS Grivory |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSG-30/4 LF 15/1 PA666-(GF+Z)45 Information provided by EMS Grivory |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSGZ-15 PA666-GF15 Product description: Grilon TSGZ-15 is a heat stabilized, normal viscosity, and impact modified PA66 + PA6 injection molding grade with 15% glass fibers. Grilon TSGZ-15 has the following important p.. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6
(Unverified Data**) 30% Glass Reinforced Toughened Polyamide 6 Zytel 73G30T BK261 is a 30% glass fiber reinforced toughened black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polym.. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN 54G15HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**) 15% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G15HSLR NC010 is a 15% glass reinforced toughened heat stabilized hydrolysis resistant high performance polyamide resin. It i.. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | ISO 527/4 |
Azdel Plus R401B02N 40% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R401B02N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m.. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | ISO 527 |
Azoty Tarnow™ TARNOFORM 300 XEC1 POM Electrically conductive, carbon fiber reinforced injection molding grade suitable for the applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe .. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | 1mm/min; ISO 527 |
BASF Ultramid® 8233G HS BK-102 33% Glass Filled PA6 (Conditioned) Ultramid 8233G HS BK-102 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature performance and d.. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | ASTM D638 |
Azdel SuperLite® SL550800-100 PP Resin Matrix / 55% Glass Fiber (1 mm Molded Thickness) AZDEL SuperLite® SL550800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | ISO 527 |
BASF Ultramid® B3WG6 CR BK 23210 15% Glass Filled (Conditioned) Description: Ultramid B3WG6 CR BK23210 s a 30% glass fiber reinforced, heat stabilized injection molding PA6 grade for crash relevant applications.Information provided by BASF |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | |
LATI Latigea B02 H6 Bio-Polymer Bio-Polymer (PLA, PHB, ...). Unfilled. Improved thermal stability. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop.. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | |
LATI Latilub 88/50-30GRT PEEK, Graphite/PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). Graphite / PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu.. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | ISO 527-1/-2 |
Lanxess Pocan® DP 7102 000000 PBT, 30% Mineral
(discontinued **) PBT, 30% mineral, injection molding, LDS |