Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.38 GPa @Temperature 175 °C |
780 ksi @Temperature 347 °F |
ISO 527-2 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep .. |
|||
Tensile Modulus | 5.38 GPa | 780 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin. Th.. |
|||
Tensile Modulus | 5.38 GPa @Temperature 23.0 °C |
780 ksi @Temperature 73.4 °F |
ISO 527-2 |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin. Th.. |
|||
Tensile Modulus | 5.38 GPa | 780 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics SABIC PPCOMPOUND G3220A PP SABIC® PPcompound G3220A is a general purpose, 20% glass filled, chemically coupled, heat stabilized homopolymer polypropylene compound. The IMDS is 209767996. |
|||
Tensile Modulus | 5.38 GPa @Temperature 175 °C |
780 ksi @Temperature 347 °F |
4; ISO 527-2 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr.. |
|||
Tensile Modulus | 5.38 GPa | 780 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA), 15% Glass Fiber (Dry) Amodel® AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin.. |
|||
Tensile Modulus | 5.38 GPa | 780 ksi | 50 mm/min; ISO 527-2/50; ASTM D638 |
Styron CALIBREâ„¢ 891-10 Polycarbonate Resin Overview: CALIBREâ„¢ 891-10 Series provides superior ignition resistance in opaque applications. The CALIBRE 891-10 series products are available in 2 additive packages: CALIBRE 891: Mold release.. |