Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.19 GPa | 753 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® NX07353 PC+ABS (Asia Pacific) Cycoloy* C7230P resin is a mineral filled, flame retardant PC/ABS. Good stiffness combined with balanced flow and impact performance, makes it a good candidate for various applications. |
|||
Tensile Modulus | 5.19 GPa | 753 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp ZZ006 PPE+PS LNP THERMOCOMP* ZZ006 is a compound based on PPE+PS Blend resin containing Milled Glass.This data was supplied by SABIC-IP for the Americas region. |