Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.03 GPa | 730 ksi | ASTM D638 |
Quadrant EPP Techtron® PSGF PPS - Compression Molded 40% Glass Reinforced Polyphenylene Sulfide (ASTM Product Data Sheet) |
|||
Tensile Modulus | 5.03 GPa | 730 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM CRS5711 PEI 15% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing. |
|||
Tensile Modulus | 5.03 GPa | 730 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM CRS5711 PEI (Asia Pacific) 15% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing. |
|||
Tensile Modulus | 5.03 GPa | 730 ksi | ASTM Test |
Styrolution Terblend® N NG-04 20% Glass Filled ABS/PA6 (Dry) Terblend N NG-04 is a glass fibre reinforced ABS/PA6 blend with excellent dimensional stability, low mold shrinkage and high heat resistance.Information provided by STYROLUTION, which is a joint ven.. |
|||
Tensile Modulus | 5.03 GPa | 730 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP WF002 PBT LNP* THERMOCOMP* WF002 is a compound based on PBT containing 10% Glass Fiber. |
|||
Tensile Modulus | 5.03 GPa | 730 ksi | ASTM D638 |
Ensinger XP-151 Compression Molded PI Compound, 15% Graphite Filled, Premium Grade The XP 150 Series are amorphous high performance polyimides with high permanent temperature and creep resistance, as well as excellent bearing and wear properties, and excellent long term thermal st.. |
|||
Tensile Modulus | 5.03 GPa @Temperature 22.8 °C |
730 ksi @Temperature 73.0 °F |
ASTM D638 |
Quadrant EPP Duratron® PAI T7530, Compression Molded Carbon Fiber Reinforced Polyamide-Imide |
|||
Tensile Modulus | 5.03 GPa @Temperature 22.8 °C |
730 ksi @Temperature 73.0 °F |
ASTM D638 |
Quadrant EPP Duratron® PAI T7530, Compression Molded Carbon Fiber Reinforced Polyamide-Imide |