Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.80 GPa | 696 ksi | |
Plastcom SLOVAMID 66 GF 14 HI TS PA66, 14% glass fibre, improved strength FeaturesChemically reinforced with 14% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. I.. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | STN EN ISO 527-2 |
Plastcom SLOVASTER® B GF 10 Polybutylene Terephthalate, 10% Glass Fiber FeaturesPBT for injection moulding, chemically reinforced with 10% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a.. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | 50 mm/min; ASTM D638 |
Ovation Polymers Opnyl OP6GF15 Nylon 6, 15% Glass Reinforced, Dry Nylon 6 - Glass reinforced (15 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. For Nylon compounds the m.. |
|||
Tensile Modulus | 4.80 GPa @Temperature 23.0 °C |
696 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
PolyOne Bergamid™ A70 GK30 black 13539126 Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | ASTM D638 |
Idemitsu Kosan Xarec® N WA 7010 SPS, 10% Glass Filled
(discontinued **) Crystalline Polymer Blend, Glass Filled. Used in Automotive Electronics applications. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | ISO 527 |
Nilit FRIANYL A63 KV35 Nylon 6.6 for injection molding, 35% glass ball reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | ISO 527-7 |
NOVA Chemicals Dylark® 378P12 Glass Reinforced Engineering Resin Features: Very high modulus, High heat resistance, excellent flow characteristics, excellent adhesion to urethaneApplications: Instrument panel substrates, Consoles, Cluster housings, Interior trim |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | ISO 527-2 |
NOVA Chemicals Dylark® 510XT Glass Reinforced Engineering Resin Features: Higher toughness product, Excellent stiffness, High heat resistance, Superior adhesion to urethane foamApplications: Instrument panel substrates, Mid-Consoles, Center Stacks, Interior tri.. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | |
LATI Latimass 82-03 D080 PA12 Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RZL36 PA 66 (Europe-Africa-Middle East) LNP* LUBRICOMP* RZL36 is a compound based on PA 66 resin containing Milled Glass, PTFE. Added features include: Internally Lubricated. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DFD02EXC PC (Europe-Africa-Middle East) LNP* Stat-kon* DFD02EXC is a compound based on Polycarbonate resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® EH7020HF PBT+PET Valox EH7020HF is a mineral filled PBT/PET that offers good surface appearance, high flow and good heat performance. EH7020HF was developed for automotive bezel application that requires basecoat + .. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® EH7020HF PBT+PET (Asia Pacific) Valox EH7020HF is a mineral filled PBT/PET that offers good surface appearance, high flow and good heat performance. EH7020HF was developped for automotiove bezel application that require basecoat +.. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® 1760E PBT+PC 11% Glass Reinforced alloy. Impact/chemical resistant. Excellent physical property retention in automotive exteriors. High flow version of Xenoy 1760 resin. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP SH0430AC_BK1D466 PA12 4.3 specific gravity nylon 12, clean compound system |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | ASTM D 638 |
Saint-Gobain Meldin® 5001 Thermoplastic Bearing Material General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin.. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | ASTM-D790 |
Polyram PlusTek PA340S6 Nylon 6.6, 30% Glass beads 30% glass beads reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | ISO 527 |
Polyram RamLloy PFS302G14 ASA/PBT Alloy, 14% Glass Fiber 14% Glass fiber reinforced ASA/PBT alloy for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | ISO 527-1/-2 |
DSM Akulon® K224-LGM35 (Cond.) 15% Glass Reinforced, 25% Mineral Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 GX 350 HWCP Combination Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSM-30/4 PA666-MD30 Information provided by EMS Grivory |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Minlon® 12TA BKB124 Nylon 66
(Unverified Data**) 32% Mineral Reinforced Toughened Polyamide 66 Minlon 12TA BKB124 is a 32% mineral reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont P.. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 80G14A NC010A Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Polyamide 66 Zytel 80G14A NC010A is a 14% glass fiber reinforced toughened high flow polyamide 66 resin. It offers outstanding performance in injection molding applica.. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide AK8ST41 PA66, Mineral Reinforced, Impact Modified, Injection Molding Staramide AK8ST41 is an Impact Modified, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide ALY430A PA66, Glass Fiber Reinforced, Injection Molding Staramide ALY430A is a Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | 1 mm/min |
Arkema Group Orgalloy® R 60T30 Nylon 6 Alloy, Mineral Filled (Conditioned) Rigid polyamide 6 alloy: easy to process, low moisture absorption, chemical resistance (no known solvents).Mineral filled. Low distortion, offers precisely dimensioned injection moldings.ISO data pr.. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® A3 GF 10 (2852) PA 6.6 Dry, 10% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics SABIC STAMAX 20YM240 PP SABIC® STAMAX 20YM240 is a 20% long glass fiber reinforced polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMDS is 62455287. |