Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.14 GPa | 600 ksi | ASTM D638 |
Quadrant EPP Duratron® PAI T4203 Extruded Polyamide-imide (ASTM Product Data Sheet) |
|||
Tensile Modulus | 4.14 GPa | 600 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ 80510 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 4.14 GPa | 600 ksi | ASTM D638 |
Fiberfil® J-60/20 Polypropylene Homopolymer, 20% Glass Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 4.14 GPa | 600 ksi | ASTM D638 |
Fiberfil® J-60/20/E Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 4.14 GPa | 600 ksi | ASTM D638 |
Fiberfil® J-60/20/E4 Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 4.14 GPa | 600 ksi | ASTM D638 |
Fiberfil® J-60/20/E8 Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 4.14 GPa | 600 ksi | ASTM D638 |
Fiberfil® J-60/20/E8/M Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 4.14 GPa | 600 ksi | ISO 527 |
Polyram PlusTek PA340S4 Nylon 66 for Injection Molding, 20% Glass-Beads Reinforced 20% Glass-beads reinforced Nylon 66 for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 4.14 GPa | 600 ksi | ASTM D638 |
Ensinger XP-150 Compression Molded Polyimide Unfilled, Premium Grade The XP 150 Series are amorphous high performance polyimides with high permanent temperature and creep resistance, as well as excellent bearing and wear properties, and excellent long term thermal st.. |
|||
Tensile Modulus | 4.14 GPa | 600 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® PE-30GF/000 WHITE High Density Polyethylene (HDPE), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedWhitePolyOne First ChoiceInformation provided by PolyOne Corporation. |