Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.13 GPa | 599 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DBP32EI PC LNP* Lubricomp* DBP32EI is a compound based on Polycarbonate resin containing 15% PTFE/Silicone and 10% Glass Bead. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 4.13 GPa | 599 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DBP32EI PC (Asia Pacific) LNP* Lubricomp* DBP32EI is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Tensile Modulus | 4.13 GPa | 599 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp DFI12E PC (Asia Pacific) LNP* Lubricomp* DFI12E is a compound based on Polycarbonate resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated, Easy Molding.This data was suppli.. |
|||
Tensile Modulus | 4.13 GPa | 599 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DFL22 PC LNP* Lubricomp* DFL22 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated. |
|||
Tensile Modulus | 4.13 GPa | 599 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DFL22 PC (Asia Pacific) LNP* Lubricomp* DFL22 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 4.13 GPa | 599 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp DFI12E PC LNP* Lubricomp* DFI12E is a compound based on Polycarbonate resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated, Easy Molding.This data was suppli.. |
|||
Tensile Modulus | 4.13 GPa | 599 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DFL12 PC LNP* Lubricomp* DFL12 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 5% PTFE. Added features include: Internally Lubricated. |
|||
Tensile Modulus | 4.13 GPa | 599 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RN001S PA 66 LNP* LUBRICOMP* RN001S is a compound based on Nylon 66 resin containing 2% MOS2. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Tensile Modulus | 4.13 GPa | 599 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RN001S PA 66 (Asia Pacific) LNP* Lubricomp* RN001S is a compound based on Nylon 66 resin containing MOS2. Added features of this material include: Internally Lubricated, Heat Stabilized. |
|||
Tensile Modulus | 4.13 GPa | 599 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS LNP* STAT-LOY* AF3009 is a compound based on ABS resin containing 10% Glass Fiber. Added features of this material include: Antistatic, Flame Retardant. |
|||
Tensile Modulus | 4.13 GPa | 599 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS (Asia Pacific) LNP* Stat-loy* AF3009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Antistat, Flame Retardant. |
|||
Tensile Modulus | 4.13 GPa | 599 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP AF002 ABS LNP THERMOCOMP* AF002 is a compound based on ABS resin containing 10% Glass Fiber. |
|||
Tensile Modulus | 4.13 GPa | 599 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP DF0029ER PC (Asia Pacific) LNP* Thermocomp* DF0029ER is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Flame Retardant. |
|||
Tensile Modulus | 4.13 GPa | 599 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP KFB11 Acetal Copoly LNP* THERMOCOMP* KFB11 is a compound based on Acetal Copolymer resin containing 5% Glass Fiber, 5% Glass Bead. Added features of this material include: Low Warpage, Chemically Coupled. |
|||
Tensile Modulus | 4.13 GPa | 599 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP MH0500C PP (Asia Pacific) LNP* Thermocomp* MH0500C is a compound based on Polypropylene resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Tensile Modulus | 4.13 GPa | 599 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT LNP* LUBRICOMP* WBL36L is a compound based on PBT resin containing 30% Glass Bead, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible. |
|||
Tensile Modulus | 4.13 GPa | 599 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT (Asia Pacific) LNP* Lubricomp* WBL36L is a compound based on Polybutylene Terephalate resin containing Glass Bead, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Tensile Modulus | 4.13 GPa | 599 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP AF002XXC ABS LNP THERMOCOMP* AF002XXC is a compound based on ABS resin containing 10% Glass Fiber. |
|||
Tensile Modulus | 4.13 GPa | 599 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP DF0029ER PC LNP* Thermocomp* DF0029ER is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Flame Retardant. |
|||
Tensile Modulus | 4.13 GPa | 599 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP MH0500C PP LNP* THERMOCOMP* MH0500C is a compound based on Polypropylene resin. Added feature of this material is: High Specific Gravity. |
|||
Tensile Modulus | 4.13 GPa | 599 ksi | Storage |
Epoxy Technology EPO-TEK® T7139 Glob Top Epoxy Product Description: EPO-TEK® T7139 is a two component, electrically insulating, encapsulating epoxy designed for semiconductor glob top applications and package assembly.Advantages & Application N.. |
|||
Tensile Modulus | 4.13 GPa | 599 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP KFB11 Acetal Copoly (Asia Pacific) LNP* Thermocomp* KFB11 is a compound based on Acetal Copolymer resin containing Glass Fiber, Milled Glass. Added features of this material include: Low Warpage, Chemically Coupled. |