Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.85 GPa | 558 ksi | |
Plastcom SLOVALEN PH 61 B 70 PP, 70% mineral filling FeaturesModified PP for injection moulding with the content of 70% of barium sulphate. Increased density. Decreased shrinkage.Used for production of vertical blind weights. Delivered in natural mode.. |
|||
Tensile Modulus | 3.85 GPa | 558 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FXE4271L PC (Asia Pacific) Lexan* FXE4271L is a 10% glass filled, impact modified polycarbonate with excellent light-shield capability. It is designed for high flow, superior surface appearance, enhance release and good impac.. |
|||
Tensile Modulus | 3.85 GPa | 558 ksi | ISO 527-2/1A/1 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and pro.. |
|||
Tensile Modulus | 3.85 GPa | 558 ksi | ISO 527-2/1A/1 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insulation.. |
|||
Tensile Modulus | 3.85 GPa | 558 ksi | 1 mm/min, Type 1A; ISO 527-2 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK) KetaSpire® KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insula.. |
|||
Tensile Modulus | 3.85 GPa | 558 ksi | 1 mm/min, Type 1A; ISO 527-2 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK) KetaSpire® KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and.. |
|||
Tensile Modulus | 3.85 GPa | 558 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
Tensile Modulus | 3.85 GPa | 558 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Europe-Africa-Middle East) Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
Tensile Modulus | 3.85 GPa | 558 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Asia Pacific) Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |